Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TIMET 75A CP Titanium (ASTM Grade 4)

Category Metal , Nonferrous Metal , Titanium Alloy , Unalloyed/Modified Titanium
Manufacturer TIMET
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TIMET 75A CP Titanium (ASTM Grade 4).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4901. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specification BS TA. 6.Features: The mechanical properties of CP titanium are influenced by small additions of oxygen and iron. By careful control of these additions, the various grades of commercially pure titanium are produced to give properties suited to different applications. TIMETAL 75A is equivalent to ASTM Grade 4. It has the highest strength of the four ASTM commercially pure titanium grades in addition to good ductility and moderate formability. The benefits of the good strength to weight ratio of TIMETAL 75A are retained at moderate temperatures. It has good impact properties at low temperatures. It can be satisfactorily welded, machined, cold worked, hot worked, and cast. It is nonmagnetic.Typical heat treatment for this alloy: Anneal at 700°C for 1 hour and air cool. Stress Relieve at 500°C for 30 mins and air cool.Data provided by TIMET.
Physical Properties Metric English Comments
Density 4.51 g/cc
0.163 lb/in³
Typical
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 680 MPa
98600 psi
Typical
Tensile Strength, Yield 560 MPa

@Strain 0.200 %
81200 psi

@Strain 0.200 %
Typical
Elongation at Break 23 %
23 %
Typical
Reduction of Area 46 %
46 %
Typical
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
Fatigue Strength 376 MPa
54500 psi
Smooth, Kt=1
Bend Radius, Minimum 3.0 t

@Thickness 2.00 mm
3.0 t

@Thickness 0.0787 in
Typical; sheet
Thermal Properties Metric English Comments
CTE, linear 8.60 µm/m-°C

@Temperature 20.0 - 100 °C
4.78 µin/in-°F

@Temperature 68.0 - 212 °F
9.50 µm/m-°C

@Temperature 20.0 - 300 °C
5.28 µin/in-°F

@Temperature 68.0 - 572 °F
9.70 µm/m-°C

@Temperature 20.0 - 425 °C
5.39 µin/in-°F

@Temperature 68.0 - 797 °F
Thermal Conductivity 16.95 W/m-K
117.6 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 425 °C
797 °F
Continuous
540 °C
1000 °F
Intermittent
Beta Transus 950 °C
1740 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe <= 0.50 %
<= 0.50 %
Nitrogen, N <= 0.050 %
<= 0.050 %
Oxygen, O <= 0.40 %
<= 0.40 %
Titanium, Ti >= 98.6 %
>= 98.6 %
Calculated as remainder
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000600 ohm-cm
0.0000600 ohm-cm
Users viewing this material also viewed the following: