Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.160 - 0.240 g/cc | 0.00579 - 0.00868 lb/in³ | Dry |
Unifrax Fiberfrax® Fibermax® Caulk Fibermax caulk is a high-temperature blend of Fiberfrax bulk fibers, Fibermax polycrystalline high-alumina fibers, and inorganic binder. This product is available in convenient-to-use caulking tube.. |
|||
Density | 0.180 - 0.240 g/cc | 0.00650 - 0.00867 lb/in³ | ISO 1183 |
Fainplast Compounds EVAtech 807I Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |