EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds
Physical Properties Metric English Comments
Density 0.180 - 0.240 g/cc
0.00650 - 0.00867 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore C 57 - 63
57 - 63
ASTM D2240
Tensile Strength at Break >= 2.50 MPa
>= 363 psi
ISO 527
Elongation at Break >= 320 %
>= 320 %
ISO 527
Thermal Properties Metric English Comments
CTE, linear 160 µm/m-°C
88.9 µin/in-°F
Shrinkage <= 2.0 %

@Temperature 70.0 °C,
Time 86400 sec
<= 2.0 %

@Temperature 158 °F,
Time 24.0 hour
Processing Properties Metric English Comments
Processing Temperature 180 - 190 °C
356 - 374 °F
Shelf Life 3.00 Month
3.00 Month
Moisture absorption after extended storage