Goodfellow Aluchrom O® Resistance Alloy

Category Metal , Electronic/Magnetic Alloy , Ferrous Metal , Superalloy , Iron Base
Manufacturer Goodfellow
Trade Name Aluchrom O®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Aluchrom O® Resistance Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resistance heating alloy with excellent resistance to oxidation at elevated temperatures. Used in many varied applications - from small household appliances to large industrial furnaces.Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 7.10 g/cc
0.257 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 650 - 1000 MPa
94300 - 145000 psi
Elongation at Break 15 %
15 %
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 20.0 - 100 °C
6.11 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 16.0 W/m-K
111 BTU-in/hr-ft²-°F
Melting Point 1520 °C
2770 °F
Maximum Service Temperature, Air 1250 °C
2280 °F
Component Elements Properties Metric English Comments
Aluminum, Al 5.0 %
5.0 %
Chromium, Cr 25 %
25 %
Iron, Fe 70 %
70 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000135 - 0.000145 ohm-cm
0.000135 - 0.000145 ohm-cm
Temperature Coefficient of 0.00007 K^-1
Curie Temperature 600 °C
1110 °F