Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.59 g/cc | 0.274 lb/in³ | |
Kennametal Stellite Delcrome® 90 Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. White cast iron, abrasion resistant. Carbide modifiers can provide a refined microstructure and.. |
|||
Density | 7.59 g/cc | 0.274 lb/in³ | Coating Property |
The NanoSteel® Company SHS 9172 HVOF Steel Alloy, Atomized Powder Coating Description: SHS 9172 HVOF is an iron based steel alloy with a nanoscale microstructure that features exceptional resistance to wear, abrasion, impact, corrosion and high temperature oxidati.. |
|||
Density | 7.59 g/cc | 0.274 lb/in³ | Weld Deposit Property |
The NanoSteel® Company SHS 9500 GMAW OAW Steel Alloy, Cored Wire Coating Description: SHS 9500 GMAW OAW is an iron based steel alloy featuring medium hardness, high toughness and high wear resistance.Key Performance Characteristics: 58-62 HRc single and double pa.. |
|||
Density | 7.59 g/cc | 0.274 lb/in³ | |
Goodfellow Cobalt/Silicon/Boron/Iron/Nickel Alloy Metallic glasses (glassy alloys) or amorphous metals. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.Information provided by Goodfellow. |
|||
Density | 7.59 g/cc | 0.274 lb/in³ | Coating Property |
The NanoSteel® Company SHS 7570 TWAS Steel Alloy, Cored Wire Coating Description: SHS 7570 TWAS is an iron based steel alloy with a nanoscale microstructure that features exceptional combined wear, impact and corrosion resistance in high chlorine, salt fog, c.. |
|||
Density | 7.58 g/cc | 0.274 lb/in³ | |
Chicago Extruded Metals BioBrass® UNS C63000 Aluminum Bronze Finished product available as bar,rod, forged, shapes, or tubes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chica.. |
|||
Density | 7.58 g/cc @Temperature 599 °C |
0.274 lb/in³ @Temperature 1110 °F |
hardened to 45 HRC |
Bohler-Uddeholm ORVAR® 2M / AISI H13 Hot Work Tool Steel Orvar 2 Microdized is a chromium-molybdenum-vanadium alloyed steelORVAR® 2M / AISI H13 is a conventionally produced hot work tool steel with overall good ductility, toughness, wear resistance, hard.. |
|||
Density | 7.58 g/cc @Temperature 599 °C |
0.274 lb/in³ @Temperature 1110 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM DIEVAR® Hot Work Tool Steel Description: Uddeholm Dievar is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross cracking, hot wear and plastic.. |
|||
Density | 7.58 g/cc @Temperature 599 °C |
0.274 lb/in³ @Temperature 1110 °F |
hardness of 56 HRC |
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are .. |
|||
Density | 7.58 g/cc @Temperature 599 °C |
0.274 lb/in³ @Temperature 1110 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Density | 7.58 g/cc @Temperature 599 °C |
0.274 lb/in³ @Temperature 1110 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Density | 7.58 g/cc @Temperature 599 °C |
0.274 lb/in³ @Temperature 1110 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM QRO® 90 SUPREME Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelQRO® 90 SUPREME is a premium hot work die steel with high hot yield strength and very good temper resistance. Especially suited for die casting of aluminum.. |
|||
Density | 7.58 g/cc @Temperature 800 °C |
0.274 lb/in³ @Temperature 1470 °F |
|
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |
|||
Density | 7.58 g/cc @Temperature 600 °C |
0.274 lb/in³ @Temperature 1110 °F |
|
Assab Steels HOTVAR Hot Work Steel HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue.. |