Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe LSSâ„¢ H13 PQ Hot Work Tool Steel TLS H13 PQ is Premium Quality H13 hot work steel that is designed to meet the highest quality standards in the die casting industry, and to excel in the most demanding hot work tooling applications... |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Industeel TENASTEEL® Cold Work Tool Steel Description: TENASTEEL is a cold work tool steel, combining a high wear resistance together with a very high toughness. Its other advantages are a good machinability in the as-delivery condition and.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe CBS-223â„¢ VIM-VAR Carburizing Bearing and Gear Steel CBS-223 VIM-VAR steel is a double vacuum melted carburizing steel with high hot hardness characteristics. Double vacuum melting sequentially combines vacuum induction melting with VACARCâ„¢ remel.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Lescalloy® 52100 VAC-ARC High Performance Bearing Steel LESCALLOY 52100 VAC-ARC is a deep hardening alloy steel used for aircraft bearings and other high stressed parts where good rolling contact fatigue strength is required at operating temperatures bel.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Lescalloy® HY-180 VIM-VAR ; 2.01 - 4.00 thickness High Strength Alloy Steel LESCALLOY HY-180 VIM-VAR steel is a high strength alloy steel with superior toughness. It is double vacuum melted (VIM-VAR vacuum induction melted followed by vacuum arc remelting) to provide superi.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Lescalloy® Jethete M-152 ESR 3" RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Crucible Steel 416R Chromium Stainless Steel Crucible 416R is a pre-hardened chromium stainless steel which is suitable for use in precision match-grade rifle barrels. It can be supplied in various hardness ranges according to the specific req.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Crucible Steel Nu-Die® V (AISI H13) Hot Work Tool Steel Nu-Die® V (AISI H13) has been the most popular, and perhaps the most versatile hot work tool steel available for many years. It provides a good balance of toughness, heat check resistance and tempe.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Crucible Steel Nu-Die® XL (Premium Quality AISI H13) Tool Steel Nu-Die XL (AISI H13) is a premium version of H13 tool steel manufactured, tested and certified to meet stringent die casting industry specifications issued by NADCA, Chrysler and others. It offers b.. |
|||
Density | 7.75 g/cc @Temperature 199 °C |
0.280 lb/in³ @Temperature 390 °F |
hardened to 57 HRC |
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel Chromium-molybdenum alloyed steelA versatile S7 grade recommended for applications demanding a high degree of toughness and moderate wear resistance. Successfully used for heavy-duty punching and sh.. |
|||
Density | 7.74 g/cc | 0.280 lb/in³ | |
AK Steel 430 ULTRA FORM® Stainless Steel 430 ULTRA FORM® Stainless Steel was developed as a more formable version of Type 430 stainless steel. It is particularly suited for parts requiring more complex shapes. 430 ULTRA FORM Stainless Ste.. |
|||
Density | 7.75 g/cc @Temperature 200 °C |
0.280 lb/in³ @Temperature 392 °F |
|
Assab Steels DF-3 Cold Work Steel DF-3 general purpose oil-hardening tool steel is a versatile manganese-chromium-tungsten steel suitable for a wide variety of cold-work applications. Its main characteristics include:Good machinabil.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum AL 13-8™ H 1100 Precipitation Hardening Alloy Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t.. |
|||
Density | 7.74 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 649°C (1200°F) Temper Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
ATI Allvac® Nickelvac® H-46 Specialty Steel, Heat Treatment: 1149°C (2100°F) Anneal Data provided by Allvac.Applications: Structural components for land-based turbine engines. Rings and structurals in jet engines. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
ATI Allvac® Vasco® X-2M Specialty Steel, Heat Treatment: 899°C (1650°F) Normalization Data provided by Allvac.Applications: High performance helicopter transmission gears, components. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
ATI Allvac® VascoJet® 1000 Specialty Steel, Heat Treatment: 1010°C (1850°F) Q+T Data provided by Allvac.Applications: Landing gear components, springs, fasteners. Gears and shafts for helicopter applications. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Carlson Nitronic® 33® Austenitic Stainless Steel General DescriptionNitronic 33 is a nitrogen-strengthened austenitic stainless steel that combines high yield strength with excellent toughness and ductility. It’s magnetic permeability remains v.. |
|||
Density | 7.75 g/cc @Temperature 200 °C |
0.280 lb/in³ @Temperature 392 °F |
|
Assab Steels 618 Plastic Mold Material ASSAB 618 is a vacuum-degassed Cr-Ni-Mo-alloy steel which is supplied in the hardened and tempered condition. ASSAB 618 is manufactured to consistently high quality standards with a controlled sulfu.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1150°F Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t.. |
|||
Density | 7.74 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 204°C Temper Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle.. |
|||
Density | 7.74 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 316°C Temper Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle.. |
|||
Density | 7.74 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 482°C Temper Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle.. |
|||
Density | 7.74 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 538°C Temper Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | H900 Condition |
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
Carpenter Custom 455® Stainless Steel, Annealed, 25 mm Bar Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Lescalloy® HY-180 VIM-VAR ; 4.01 - 8.00 thickness High Strength Alloy Steel LESCALLOY HY-180 VIM-VAR steel is a high strength alloy steel with superior toughness. It is double vacuum melted (VIM-VAR vacuum induction melted followed by vacuum arc remelting) to provide superi.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Lescalloy® Jethete M-152 ESR 6" RCS High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800°.. |
|||
Density | 7.75 g/cc @Temperature 191 °C |
0.280 lb/in³ @Temperature 375 °F |
hardened to 62 HRC |
Bohler-Uddeholm O1 Cold Work Tool Steel Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface ha.. |