Category Metal , Ferrous Metal , Carbon Steel , High Carbon Steel , Tool Steel
Manufacturer Groupe Arcelor
Trade Name TENASTEEL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel TENASTEEL® Cold Work Tool Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TENASTEEL is a cold work tool steel, combining a high wear resistance together with a very high toughness. Its other advantages are a good machinability in the as-delivery condition and a particularly high resistance to thermal softening. The steel is delivered in the soft annealed condition with a maximum hardness of 250 HB. TENASTEEL is specially designed to replace D2 type steels widely used by toolmakers but suffering from an excessive brittleness. Thanks to its chemistry increasing resistance to softening during tempering, TENASTEEL is especially suited for all processes of surface treatment and coatings commonly used in the market, including nitriding processes involving high temperatures.Information provided by manufacturer.
Physical Properties Metric English Comments
Density 7.75 g/cc
0.280 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell <= 250
<= 250
Typical in annealed condition
Hardness, Rockwell C 60
60
Heat Treated
Modulus of Elasticity 205 GPa
29700 ksi
Typical
Compressive Strength 2300 MPa
334000 psi
Typical
Charpy Impact, Unnotched 25.0 J
18.4 ft-lb
Typical
Thermal Properties Metric English Comments
CTE, linear 10.2 µm/m-°C

@Temperature 20.0 - 100 °C
5.67 µin/in-°F

@Temperature 68.0 - 212 °F
11.3 µm/m-°C

@Temperature 20.0 - 200 °C
6.28 µin/in-°F

@Temperature 68.0 - 392 °F
11.9 µm/m-°C

@Temperature 20.0 - 300 °C
6.61 µin/in-°F

@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 20.0 °C
0.110 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 21.0 W/m-K

@Temperature 20.0 °C
146 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Carbon, C 1.0 %
1.0 %
Chromium, Cr 7.5 %
7.5 %
Iron, Fe 88.245 - 88.25 %
88.245 - 88.25 %
As remainder
Manganese, Mn 0.35 %
0.35 %
Molybdenum, Mo 2.6 %
2.6 %
Sulfur, S <= 0.0050 %
<= 0.0050 %
Vanadium, V 0.30 %
0.30 %
Users viewing this material also viewed the following: