Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Latrobe LSSâ„¢ H13 PQ Hot Work Tool Steel

Category Metal , Ferrous Metal , Alloy Steel , Tool Steel , Hot Work Steel
Manufacturer Latrobe Steel
Trade Name LSS™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe LSSâ„¢ H13 PQ Hot Work Tool Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TLS H13 PQ is Premium Quality H13 hot work steel that is designed to meet the highest quality standards in the die casting industry, and to excel in the most demanding hot work tooling applications. TLS H13 PQ is melted using an electric-arc furnace, is refined by the argon-oxygen-decarburization (AOD) process, and is further enhanced to aerospace quality levels using Vacuum-Arc or Electro-Slag Remelting. These special melting practices along with special thermo-mechanical and annealing treatments result in ultra-high microcleanliness and a homogeneous, fine-grained microstructure.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.75 g/cc
7.75 g/cc
Density 7.75 g/cc
0.280 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 50
50
Air Cooled from 982°C, 30 minutes
52.5
52.5
Air Cooled from 1010°C, 30 minutes
54
54
Air Cooled from 1032°C, 30 minutes
Modulus of Elasticity 207 GPa
30000 ksi
159 GPa

@Temperature 538 °C
23000 ksi

@Temperature 1000 °F
186 GPa

@Temperature 204 °C
27000 ksi

@Temperature 400 °F
Machinability 65 - 70 %
65 - 70 %
1% Carbon Steel
Charpy Impact 13.6 J
10.0 ft-lb
V-Notch; Air Cooled from 1024°C; 535°C Temper Temperature
32.5 J
24.0 ft-lb
V-Notch; Air Cooled from 1024°C; 640°C Temper Temperature
35.3 J
26.0 ft-lb
V-Notch; Air Cooled from 1024°C; 260°C Temper Temperature
Thermal Properties Metric English Comments
CTE, linear 11.3 µm/m-°C

@Temperature 21.0 - 204 °C
6.28 µin/in-°F

@Temperature 69.8 - 399 °F
13.5 µm/m-°C

@Temperature 21.0 - 538 °C
7.50 µin/in-°F

@Temperature 69.8 - 1000 °F
Thermal Conductivity 17.6 W/m-K

@Temperature 27.0 °C
122 BTU-in/hr-ft²-°F

@Temperature 80.6 °F
23.4 W/m-K

@Temperature 204 °C
162 BTU-in/hr-ft²-°F

@Temperature 399 °F
26.8 W/m-K

@Temperature 649 °C
186 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Component Elements Properties Metric English Comments
Carbon, C 0.40 %
0.40 %
Chromium, Cr 5.25 %
5.25 %
Iron, Fe 90.599 %
90.599 %
Manganese, Mn 0.40 %
0.40 %
Molybdenum, Mo 1.35 %
1.35 %
Silicon, Si 1.0 %
1.0 %
Sulfur, S 0.0010 %
0.0010 %
Vanadium, V 1.0 %
1.0 %
Chemical Properties Metric English Comments
Critical Temperature 802 °C
1480 °F
Ar1
826 °C
1520 °F
Ar3
840 °C
1540 °F
Ac1
890 °C
1630 °F
Ac3
Users viewing this material also viewed the following: