Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.77 g/cc | 0.317 lb/in³ | |
Kennametal Stellite Stellite® 33 Completely non-magnetic. Specific Electrical Resistance: 39.8 µOhm/in^3.Applications: standard tool bits, tipped tools, form tools, milling cutter blades, wood working tools, reamer blades, cut-o.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | |
Indium Corp. Indalloy 212 Ag-Cu-Zn-Cd Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.78 g/cc | 0.317 lb/in³ | |
Indium Corp. Indalloy 95 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | |
Indium Corp. Indalloy 98 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | |
Special Metals NILOMAG® Alloy 77 A nickel-iron alloy with additions of copper and molybdenum. It is a low-loss, soft-magnetic alloy with a high initial permeability. Initial permeability 60,000; maximum permeability 300,000; satu.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | Annealed |
Eagle Brass 425 Tin Brass 2%, 1/2 Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | Annealed |
Eagle Brass 425 Tin Brass 2%, 1/4 Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | Annealed |
Eagle Brass 425 Tin Brass 2%, 3/4 Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | Annealed |
Eagle Brass 425 Tin Brass 2%, Annealed Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | Annealed |
Eagle Brass 425 Tin Brass 2%, Extra Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | Annealed |
Eagle Brass 425 Tin Brass 2%, Extra Spring Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | Annealed |
Eagle Brass 425 Tin Brass 2%, Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | Annealed |
Eagle Brass 425 Tin Brass 2%, Spring Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | Annealed |
Eagle Brass 64725 MAX251C, 1/2 Hard Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | Annealed |
Eagle Brass 64725 MAX251C, Extra Hard Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | Annealed |
Eagle Brass 64725 MAX251C, Extra Spring Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | Annealed |
Eagle Brass 64725 MAX251C, Hard Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | Annealed |
Eagle Brass 64725 MAX251C, Spring Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | |
CLAL-MSX NICLAL 38 Copper Alloy Description: Niclal 38 is a precision resistance alloy, with moderate Resistivity, low Temperature coefficient of resistance and low thermal EMF versus Copper. With high stability of electrical resi.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | |
Chicago Extruded Metals BioBrass® UNS C22600 Copper-Zinc Alloy Finished product available as bar or wire.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metal.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | |
Cadi 2 MOLD-MOR™ A very hard heat treatable beryllium-copper alloy with moderate electrical conductivity. C17510 can be utilized when a combination of very good mechanical strength along with moderate electrical an.. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | |
Cadi 20 MOLD-MOR™ A Beryllium Copper Alloy with high thermal conductivity and moderate hardness.Information provided by Cadi Company. |
|||
Density | 8.77 g/cc | 0.317 lb/in³ | |
ATI Allvac® Nickelvac® H-N Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal Data provided by Allvac.Applications: Turbine gas sealing components. |
|||
Density | 8.78 g/cc | 0.317 lb/in³ | |
Indium Corp. Indalloy 45 Bismuth Solder Alloy Information Provided by Indium Corporation |