Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 4508 Single-Coated Foam Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 4508 Single-Coated Foam Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plasticized) as tape adhesion is typically satisfactory within 20 minutes and continues to build and additional time.Information provided by 3M
Physical Properties Metric English Comments
Density 0.320 g/cc
0.0116 lb/in³
foam with adhesive; ASTM D3574
Water Absorption 5.0 %
5.0 %
ASTM D1056
Thickness 76.2 microns
3.00 mil
Release Liner
3180 microns
125 mil
Total
Mechanical Properties Metric English Comments
Hardness, Shore OO 50
50
Foam with adhesive; ASTM D2240
Tensile Strength at Break 0.690 MPa
100 psi
Die "A"; ASTM D3759
Elongation at Break 200 %
200 %
Die "A"; ASTM D3759
Compressive Strength 0.0276 MPa
4.00 psi
Deflection, Compress 25%; ASTM D3574
Compression Set 15 %
15 %
ASTM D1667
Thermal Properties Metric English Comments
Thermal Conductivity 0.0430 W/m-K
0.298 BTU-in/hr-ft²-°F
ASTM C518
Electrical Properties Metric English Comments
Surface Resistivity per Square 4.00e+10 ohm
4.00e+10 ohm
Non-adhesive side; ASTM D257
1.00e+11 ohm
1.00e+11 ohm
Adhesive side; ASTM D257
Dielectric Strength 3.94 kV/mm
100 kV/in
ASTM D149
Descriptive Properties Value Comments
Adhesive Type 430
Appearance Black
White
liner
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved