Polymer Property : Density = 0.574 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density >= 15.9 g/cc
>= 0.574 lb/in³
Hogen H40W 85 Tungsten/15 Copper PM Metal Composite
Fully heat treated.Hogen refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Data provided by Hogen Industries.
Density >= 15.9 g/cc
>= 0.574 lb/in³
Mi-Tech Metals Thermitechâ„¢ CW85 85 Tungsten/15 Copper PM Metal Composite
Fully heat treated.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Data provided by Mi-Tech Metals.
Density 15.9 g/cc
0.574 lb/in³
Wieland Portadur T Casting Alloy
Gold casting alloyApplications: inlays/onlays, crowns, acrylic veneeringDental
Density 15.9 g/cc
0.574 lb/in³
Williams Advanced Alloys C110 Solder
Williams extensive offering of Contact Alloys are cast and fabricated to meet the exacting standards of various micro electronics applications. All Williams electrical contact alloys are available i..