Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 15.9 g/cc | >= 0.574 lb/in³ | |
Hogen H40W 85 Tungsten/15 Copper PM Metal Composite Fully heat treated.Hogen refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Data provided by Hogen Industries. |
|||
Density | >= 15.9 g/cc | >= 0.574 lb/in³ | |
Mi-Tech Metals Thermitechâ„¢ CW85 85 Tungsten/15 Copper PM Metal Composite Fully heat treated.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Data provided by Mi-Tech Metals. |
|||
Density | 15.9 g/cc | 0.574 lb/in³ | |
Wieland Portadur T Casting Alloy Gold casting alloyApplications: inlays/onlays, crowns, acrylic veneeringDental |
|||
Density | 15.9 g/cc | 0.574 lb/in³ | |
Williams Advanced Alloys C110 Solder Williams extensive offering of Contact Alloys are cast and fabricated to meet the exacting standards of various micro electronics applications. All Williams electrical contact alloys are available i.. |