Physical Properties Metric English Comments
Density 0.820 - 0.880 g/cc
0.0296 - 0.0318 lb/in³
fired density (compressed)
Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications
Insural® 85 MASTIC is an asbestos-free, durable and insulating refractory composition designed for the fabrication of launders and jointing, bedding and patching of precast refractory shapes.Advant..
Density 0.820 - 0.880 g/cc
0.0296 - 0.0318 lb/in³
fired density (compressed)
Pyrotek Insural® GP MASTIC Insulating mastic for general-purpose refractory applications
Insural® GP Mastic is an asbestos-free, durable and insulating refractory fiber composition designed for general-purpose patching and veneering applications that are not exposed to contact with mol..
Density 0.820 - 4.20 g/cc
0.0296 - 0.152 lb/in³
Average value: 1.29 g/cc Grade Count:210
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va..
Density 0.820 - 0.820 g/cc

@Temperature 240 - 240 °C
0.0296 - 0.0296 lb/in³

@Temperature 464 - 464 °F
Average value: 0.820 g/cc Grade Count:1
Overview of materials for Nylon 612, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app..
Density 0.820 - 11.0 g/cc
0.0296 - 0.397 lb/in³
Average value: 1.42 g/cc Grade Count:484
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Density >= 0.820 g/cc

@Temperature 20.0 °C
>= 0.0296 lb/in³

@Temperature 68.0 °F
Kazanorgsintez E-12 Petroleum Resin
Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic ..
Density 0.820 g/cc
0.0296 lb/in³
ASTM D1475-85
Lord Adhesives Aeroglaze® 9953 Epoxy Primer Thinner
Aeroglaze® 9953 thinner is used to reduce Aeroglaze epoxy viscosity for spray applicationsAll information provided by Lord.
Density 0.820 - 0.845 g/cc

@Temperature 15.0 °C
0.0296 - 0.0305 lb/in³

@Temperature 59.0 °F
Unipetrol Grade B Diesel Oil
Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap..
Density 0.820 - 0.845 g/cc

@Temperature 15.0 °C
0.0296 - 0.0305 lb/in³

@Temperature 59.0 °F
Unipetrol Grade D Diesel Oil
Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap..
Density 0.820 g/cc
0.0296 lb/in³
ConocoPhillips Syncon® 22 Synthetic AW Hydraulic Fluid 22
Syncon AW Hydraulic Fluid is a premium quality, synthetic antiwear hydraulic fluid developed for use in industrial and mobile equipment operating at extreme temperatures. It is particularly recommen..
Density 0.820 g/cc
0.0296 lb/in³
DuPont™ Nomex® N196 Paper, 10 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Density 0.820 g/cc
0.0296 lb/in³
DuPont™ Nomex® N196 Paper, 7 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Density 0.820 g/cc
0.0296 lb/in³
Calculated number using basis weight and thickness
DuPont™ Nomex® Type 993, 120 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..
Density 0.820 g/cc
0.0296 lb/in³
Calculated number using basis weight and thickness
DuPont™ Nomex® Type 993, 160 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..
Density 0.820 g/cc

@Temperature 15.6 °C
0.0296 lb/in³

@Temperature 60.1 °F
ASTM D4052
ExxonMobil SpectraSyn Plus™ 4 Advanced Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn Plus™ Advanced Polyalphaolefin (PAO) provide an optimal combination of volatility and low-temperature fluidity. SpectraSyn Plus™ Advanced products viscosity indices..
Density 0.820 g/cc

@Temperature 15.6 °C
0.0296 lb/in³

@Temperature 60.1 °F
ASTM D4052
ExxonMobil SpectraSyn™ 4 Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) ..
Density 0.820 g/cc
0.0296 lb/in³
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612  (Unverified Data**)
Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers
Density 0.820 g/cc
0.0296 lb/in³
ASTM C134
BNZ Materials BNZP-26 Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Density 0.820 g/cc
0.0296 lb/in³
ASTM C134
BNZ Materials Color A Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Density 0.820 g/cc
0.0296 lb/in³
3M 4412G Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
Density 0.820 g/cc
0.0296 lb/in³
BASF N-Ethylpiperidine
Formula: C7H13NCAS: 766-09-6Description: N-Ethylpiperidine is a colorless to yellow liquid, with an amine-like odor characteristic with this product. It is miscible with water.Synonyms: EPIP, 1-Eth..
Density 0.820 g/cc
0.0296 lb/in³
Sintered; ASTM D792
ALM PA-640-GSL Filled Nylon 12 Prototyping Polymer
This carbon fiber/glass sphere filled composite is an easy to process, extremely light weight filled PA 12 material.Improved dimensional stability, recyclability, and increased stiffness.Good Z dire..
Density 0.820 g/cc
0.0296 lb/in³
3M 4411B Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
Density 0.820 g/cc
0.0296 lb/in³
3M 4411G Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
Density 0.820 g/cc
0.0296 lb/in³
3M 4411N Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
Density 0.820 g/cc
0.0296 lb/in³
3M 4412N Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
Density 0.820 - 0.845 g/cc

@Temperature 15.0 °C
0.0296 - 0.0305 lb/in³

@Temperature 59.0 °F
Unipetrol Grade F Diesel Oil
Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap..