Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Pyrotek, Inc.
Trade Name Insural®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Insural® 85 MASTIC is an asbestos-free, durable and insulating refractory composition designed for the fabrication of launders and jointing, bedding and patching of precast refractory shapes.AdvantagesUser-friendly workability Low shrinkage reduces pull-out from joints High strength reduces the risk of erosion of repaired areas and joints Not wetted by molten aluminum Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.820 - 0.880 g/cc
0.0296 - 0.0318 lb/in³
fired density (compressed)
1.45 - 1.55 g/cc
0.0524 - 0.0560 lb/in³
wet density (as supplied)
Loss On Ignition 35 - 40 %
35 - 40 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00350 - 0.00400 GPa
0.508 - 0.580 ksi
dried 24 hours @ 120°C
0.00280 - 0.00350 GPa

@Treatment Temp. 750 °C,
Time 86400 sec
0.406 - 0.508 ksi

@Treatment Temp. 1380 °F,
Time 24.0 hour
Thermal Properties Metric English Comments
Thermal Conductivity 0.160 W/m-K

@Temperature 200 °C
1.11 BTU-in/hr-ft²-°F

@Temperature 392 °F
0.200 W/m-K

@Temperature 400 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 752 °F
0.240 W/m-K

@Temperature 650 °C
1.67 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Maximum Service Temperature, Air 1000 °C
1830 °F
Continuous
Shrinkage <= 1.00 %

@Temperature 120 °C,
Time 86400 sec
<= 1.00 %

@Temperature 248 °F,
Time 24.0 hour
<= 2.00 %

@Temperature 750 °C,
Time 86400 sec
<= 2.00 %

@Temperature 1380 °F,
Time 24.0 hour
fired 24 hours @ 750°C
<= 2.50 %

@Temperature 1000 °C,
Time 86400 sec
<= 2.50 %

@Temperature 1830 °F,
Time 24.0 hour
fired 24 hours @ 1000°C
Component Elements Properties Metric English Comments
Al2O3 20 %
20 %
SiO2 75 %
75 %
Descriptive Properties Value Comments
72 Hour Cup Test 7075 Alloy No Reaction / Excellent
815°C
Users viewing this material also viewed the following: