Polymer Property : Density = 0.906 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.906 g/cc
0.0327 lb/in³
ASTM D792
Lushan PJ-1 Polypropylene Compounds for Steel Pipe Top Coats
Polypropylene compound for steel pipe top coats Lushan PJ-1 is used for 3LPP coating system in colored white. It is supplied in pellets for melt extrusion or in a powder for application by spray or ..
Density 0.906 g/cc
0.0327 lb/in³
ISO 1183
Borealis BB125MO Polypropylene Copolymer
BB125MO is a heterophasic copolymer. This grade is a low melt flow rate grade intended for blow molding and sheet extrusion, and features extremely good process ability with improved melt strength a..
Density 0.906 g/cc
0.0327 lb/in³
ISO 1183
Borealis BJ356MO Polypropylene Copolymer
BJ356MO is a heterophasic copolymer. This grade provides very high melt flow rate, very high stiffness and medium impact strength. and is designed for high-speed injection molding and contains nucle..
Density 0.906 g/cc
0.0327 lb/in³
ISO 1183
Borealis BJ360MO Polypropylene Copolymer
BJ360MO is a heterophasic copolymer. This grade provides unique combination of very high melt flow rate, high impact strength and stiffness. and is designed for high-speed injection molding and cont..
Density 0.906 g/cc
0.0327 lb/in³
ISO 1183
Borealis BJ380MO Polypropylene Copolymer
BJ380MO is a very high melt flow heterophasic copolymer with high/medium impact strength and stiffness. This grade is designed for high-speed injection molding and contains nucleating and antistatic..
Density 0.906 g/cc
0.0327 lb/in³
ISO 1183
Borealis BorPURE™ RG466MO Polypropylene, Transparent Random Copolymer
BorPure™ RG466MO is a specially modified high MFR transparent polypropylene random copolymer based on proprietary Borealis Nucleation Technology (BNT), with an excellent organoleptic performance. N..
Density 0.906 g/cc
0.0327 lb/in³
ISO 1183
Borealis RG460MO Polypropylene, Transparent Random Copolymer
RG460MO is a specially modified transparent polypropylene random copolymer with high melt flow. and is designed for high-speed injection molding and contains nucleating and demolding additives. Pro..
Density 0.906 g/cc
0.0327 lb/in³
ASTM D1505
Westlake Mxsten CV77512 Polyethylene Plastomer
Mxsten CV plastomer CV77512 is a polyethylene plastomer designed for blown film extrusion that contains high slip, high antiblock and high processing aid additives. Films produced with this resin ex..
Density 0.906 g/cc
0.0327 lb/in³
ASTM-D4883
Westlake Mxsten CV77519 Polyethylene Plastomer
Mxsten CV Plastomer CV77519 is a polyethylene plastomer designed for blown film extrusion that contains no slip and no antiblock. It does contain high processing aid. Films produced with this resin ..
Density 0.906 g/cc
0.0327 lb/in³
ASTM D1505
Westlake Mxsten CV77523 Polyethylene Plastomer
Mxsten CV plastomer CV77523 is a polyethylene plastomer designed for blown film extrusion that contains high slip, very high antiblock and polymer processing aid additives. Films produced with this ..
Density 0.906 g/cc
0.0327 lb/in³
ASTM D1505
Westlake Mxsten CV77529 Polyethylene Plastomer
Mxsten CV plastomer CV77529 is a polyethylene plastomer designed for blown film extrusion that contains high slip, very high antiblock and polymer processing aid additives. Films produced with this ..
Density 0.906 g/cc
0.0327 lb/in³
ASTM D1505
Bapolene® 4052F Polypropylene, Blown Film Grade
Bapolene PP4052F is a PP homopolymer for blown film applications. It contains slip and antiblock additives as processing aids. It offers good clarity and optical properties. This product meets FD..
Density 0.906 g/cc
0.0327 lb/in³
ASTM D1505
Amco PRIMATOP PP HOMO 120 Injection Molding Polypropylene
Features:medium viscosityexcellent processabilitygood stiffnessenvironmental stress crack resistanceheat performanceminimal odor and tasteApplications:closuressmall applianceshousewarestoyscontains ..