Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bapolene® 4052F Polypropylene, Blown Film Grade

Category Polymer , Film , Thermoplastic , Polypropylene (PP)
Manufacturer Bapolene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 4052F Polypropylene, Blown Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene PP4052F is a PP homopolymer for blown film applications. It contains slip and antiblock additives as processing aids. It offers good clarity and optical properties. This product meets FDA standards for food contact applications.Applications: Film and sheetBapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.906 g/cc
0.0327 lb/in³
ASTM D1505
Water Absorption <= 0.010 %
<= 0.010 %
ASTM D-570
Linear Mold Shrinkage 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
ASTM D-955
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 101
101
ASTM D-785
Tensile Strength, Yield 37.2 MPa
5400 psi
2 in/min (50 mm/min); ASTM D-638
Elongation at Break 78 %
78 %
2 in/min (50 mm/min); ASTM D-638
Elongation at Yield 8.0 %
8.0 %
2 in/min (20 mm/min); ASTM D-638
Flexural Modulus 1.53 GPa
222 ksi
Secant @ 1% strain; ASTM D-790
Izod Impact, Notched 0.270 J/cm
0.506 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C
226 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 218 - 260 °C
424 - 500 °F
Descriptive Properties Value Comments
Process Film
Region Europe/Turkey
International
Users viewing this material also viewed the following: