Polymer Property : Density = 1.043 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.043 g/cc
0.03768 lb/in³
Lucite International Elvacite ® 2550 Acrylic Resin
Elvacite® 2550 is a solid bead methacrylate copolymer resin. It is designed to provide excellent adhesion to metal surfaces and is a resin with good flexibility and medium molecular weight. As su..
Density 1.043 g/cc
0.03768 lb/in³
ISO 1183
Styrolution Polystyrol 143 E GR 2 PS
Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b..
Density 1.043 g/cc
0.03768 lb/in³
ISO 1183
Styrolution Polystyrol 143 E GR 21 PS
Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b..
Density 1.043 g/cc
0.03768 lb/in³
BASF N-Vinyl-2-pyrrolidone, Non-Stabilized
Formula: C6H9NOCAS: 88-12-0Description: Vinyl pyrrolidone is a colorless to yellowish liquid, with a characteristic odor. It is miscible in water and organic solvents.Synonyms: N-Vinylpyrrolidone, ..
Density 1.043 g/cc
0.03768 lb/in³
ASTM D792-ISO 1183
DuPont Surlyn® SURSG201UG  (discontinued **)
Surlyn Reflections® SG201UG is a modified ionomer resin for applications that require a high gloss, molded in color surface finish directly from the mold. The material is weatherable, durable and p..