Eurotec® Tecomid® NB40 GR25 NL PA6, 25% glass fiber reinforced, natural

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Eurotec
Trade Name Tecomid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurotec® Tecomid® NB40 GR25 NL PA6, 25% glass fiber reinforced, natural.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Eurotec®
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Moisture Absorption 2.20 %

@Temperature 23.0 °C
2.20 %

@Temperature 73.4 °F
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
Eurotec
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
Eurotec
Mechanical Properties Metric English Comments
Tensile Strength at Break 160 MPa
23200 psi
ISO 527
Elongation at Break 3.5 %
3.5 %
ISO 527
Tensile Modulus 8.50 GPa
1230 ksi
ISO 527
Izod Impact, Notched (ISO) 11.0 kJ/m²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
13.0 kJ/m²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO) 70.0 kJ/m²

@Temperature -30.0 °C
33.3 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
[10 K/min], ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75
Vicat Softening Point 210 °C

@Load 5.10 kg
410 °F

@Load 11.2 lb
ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Comparative Tracking Index 500 V
500 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Processing Temperature 250 - 270 °C
482 - 518 °F
Feed Temperature 60.0 - 80.0 °C
140 - 176 °F
Throat
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Moisture Content <= 0.20 %
<= 0.20 %
ISO 960
Hold Pressure 50.0 - 100 MPa
7250 - 14500 psi
Descriptive Properties Value Comments
Back Pressure Low
Injection Speed Fast
Users viewing this material also viewed the following: