Polymer Property : Density = 1.59 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.27 - 1.59 g/cc
0.0459 - 0.0574 lb/in³
Average value: 1.38 g/cc Grade Count:11
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum ..
Density 1.56 - 1.59 g/cc
0.0564 - 0.0574 lb/in³
Average value: 1.58 g/cc Grade Count:3
Overview of materials for Phenolic, Resole, Mineral/Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v..
Density 1.55 - 1.59 g/cc
0.0560 - 0.0574 lb/in³
ISO R 1184
Fainplast Compounds RK 325 Rigid PVC, Extrusion Lead Free
Verticle curtains
Density 1.49 - 1.59 g/cc
0.0538 - 0.0574 lb/in³
Trelleborg Offshore Vikotherm™ 73785 Insulative Elastomer
Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res..
Density 1.55 - 1.59 g/cc
0.0560 - 0.0574 lb/in³
ISO R 1183
Fainplast Compounds AP 86 Flexible PVC, Flame Retardant Insulation
General purposes
Density 1.55 - 1.59 g/cc
0.0560 - 0.0574 lb/in³
ISO R 1183
Fainplast Compounds GK 88 Flexible PVC, Flame Retardant Sheathing Lead Free
General purposes
Density 1.55 - 1.59 g/cc
0.0560 - 0.0574 lb/in³
ISO R 1183
Fainplast Compounds GA 82 Flexible PVC, Flame Retardant Sheathing
General purposes
Density 1.55 - 1.59 g/cc
0.0560 - 0.0574 lb/in³
ISO R 1183
Fainplast Compounds GA 86 Flexible PVC, Flame Retardant Sheathing
General purposes