Fainplast Compounds AP 86 Flexible PVC, Flame Retardant Insulation

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds AP 86 Flexible PVC, Flame Retardant Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purposes
Physical Properties Metric English Comments
Density 1.55 - 1.59 g/cc
0.0560 - 0.0574 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 84 - 88
84 - 88
ISO R 868
Tensile Strength at Break >= 12.0 MPa
>= 1740 psi
ISO R 527
Elongation at Break >= 240 %
>= 240 %
ISO R 527
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+13 ohm-cm

@Temperature 23.0 °C
2.00e+13 ohm-cm

@Temperature 73.4 °F
ASTM D257
Descriptive Properties Value Comments
Thermal Stability (minutes) 70
CEI 20-34/3-2