Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.61 g/cc | 0.275 lb/in³ | Sintered |
Kinetics MIM 2.5% SiFe Soft Magnetic Steel Low alloy steel, silicon. A work hardenable steel alloy that offers very good magnetic properties, tensile strength, hardness, wear resistance, and increased spring steel strength. Can be plated or .. |
|||
Density | 7.61 g/cc | 0.275 lb/in³ | Sintered |
Kinetics MIM 420 Stainless Steel (Oil Quench Heat Treat) Martensitic stainless steel. Very good strength, hardness, and wear resistance while offering some corrosion resistance. Magnetic. Higher hardness typical with oil quench over that of vacuum heat t.. |
|||
Density | 7.61 g/cc | 0.275 lb/in³ | Sintered |
Kinetics MIM 420 Stainless Steel (Vacuum Heat Treat) Martensitic stainless steel. Very good strength, hardness, and wear resistance while offering some corrosion resistance. Magnetic. Less distortion typically with vacuum heat treat over that of oil q.. |
|||
Density | 7.61 g/cc | 0.275 lb/in³ | |
Latrobe DuraTechâ„¢ 20CV Powder Metal Stainless Tool Steel DuraTech 20CV is a highly wear resistant, powder metallurgy stainless tool steel. The steel contains a large volume of extremely hard vanadium carbides, which provide excellent wear resistance. Du.. |
|||
Density | 7.61 g/cc | 0.275 lb/in³ | |
Schmolz + Bickenbach 430FR Stainless Steel Bar Description: Ugitech’s 430FR is a ferritic stainless steel designed for soft magnetic components operating in corrosive environments. The 17.00% - 18.00% chromium makes corrosion resistance sim.. |
|||
Density | 7.61 g/cc @Temperature 399 °C |
0.275 lb/in³ @Temperature 750 °F |
hardened to 62 HRC |
Bohler-Uddeholm AISI A2 Cold Work Tool Steel Description: AISI A2 is an air- or oil hardening chromiummolybdenum-vanadium alloyed tool steel characterized byAISI A2 is characterized by: Good machinability High stability after hardening High c.. |
|||
Density | 7.61 g/cc @Temperature 399 °C |
0.275 lb/in³ @Temperature 750 °F |
hardened to 62 HRC |
Bohler-Uddeholm AISI D2 Cold Work Tool Steel AISI D2 is a high-carbon, high-chromium tool steel alloyed with molybdenum and vanadiumAISI AD2 is characterized by: High wear resistance High compressive strength Good through-hardening properties.. |
|||
Density | 7.61 g/cc | 0.275 lb/in³ | |
AK Steel 11 Cr-Cb™ Ferritic Stainless steel AK Steel 11 Cr-Cb™ has increased silicon levels and is dual stabilized with titanium and columbium. Designed for use in automotive exhaust tubing and other high-temperature applications, this is a.. |
|||
Density | 7.61 g/cc | 0.275 lb/in³ | |
AK Steel 409 Ferritic Stainless steel AK Steel 409 Stainless Steels are especially useful for applications where oxidation or corrosion protection beyond the capacity of carbon steel and some coated steels is needed. Current applicatio.. |
|||
Density | 7.61 g/cc @Temperature 400 °C |
0.275 lb/in³ @Temperature 752 °F |
|
Assab Steels ASSAB 88 Cold Work Steel ASSAB 88 (SLEIPNER) is a chromium-molybdenum-vanadium alloyed tool steel which is characterized by:Good wear resistanceGood chipping resistanceHigh compressive strengthHigh hardness (>60HRC) after h.. |
|||
Density | 7.61 g/cc @Temperature 400 °C |
0.275 lb/in³ @Temperature 752 °F |
|
Assab Steels ASSAB XW-41 Cold Work Steel XW-41 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength Good through-hardening propertiesHigh stability i.. |
|||
Density | 7.61 g/cc @Temperature 400 °C |
0.275 lb/in³ @Temperature 752 °F |
|
Assab Steels ASSAB XW-42 Cold Work Steel XW-42 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength High hardness after hardeningGood through-hardeni.. |
|||
Density | 7.61 g/cc @Temperature 400 °C |
0.275 lb/in³ @Temperature 752 °F |
|
Assab Steels ASSAB XW-5 Cold Work Steel ASSAB XW-5 is a high-carbon, high chromium tool steel alloyed with tungsten, characterized by:High wear resistanceHigh compressive strengthHigh surface hardness after hardeningGood through-hardening.. |
|||
Density | 7.61 g/cc | 0.275 lb/in³ | |
ATI Allegheny Ludlum AL 453™ Stainless Steel Single phase iron-chromium ferritic stainless steel alloy. Should be annealed between 1450 and 1600°F and quickly cooled. Information provided by Allegheny Ludlum |
|||
Density | 7.61 g/cc | 0.275 lb/in³ | |
Latrobe LSS™ 440C Stainless Steel Knife (ASTM A276) TLS 440C Stainless Knife Steel is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 60 HRC. The high carbon content results in a hard matrix and numero.. |