Physical Properties Metric English Comments
Density 7.62 g/cc
0.275 lb/in³
Sintered
Kinetics MIM 12 Chrome
Stainless Steel for soft magnetic applications. Information provided by Kinetics, Inc.
Density 7.62 g/cc
0.275 lb/in³
Indium Corp. Indalloy 253 Indium Solder Alloy
Information Provided by Indium Corporation
Density 7.62 g/cc
0.275 lb/in³
Indium Corp. Indalloy 211 Ag-Cu Solder Alloy
Information Provided by Indium Corporation
Density 7.62 g/cc
0.275 lb/in³
Carlson Nitronic® 60® Austenitic Stainless Steel
General DescriptionNitronic 60 is an anti-galling and wear resistant austenitic stainless steel. It provides a significantly lower cost alternative to combat wear and galling when compared with cob..
Density 7.62 g/cc
0.275 lb/in³
HP Alloys Nitronic® 60 Austenitic Stainless, Level 1 Cold Worked
Level 1 Cold Worked applies to tensile properties of 0.25 to 4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was origin..
Density 7.62 g/cc
0.275 lb/in³
HP Alloys Nitronic® 60 Austenitic Stainless, Level 2 Cold Worked
Level 2 Cold Worked applies to tensile and hardness properties of 0.25 to 4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic all..
Density 7.62 g/cc
0.275 lb/in³
HP Alloys Nitronic® 60 Austenitic Stainless, Level 3 Cold Worked
Level 3 Cold Worked applies to tensile properties of 0.25 to 2.4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was orig..
Density 7.62 g/cc
0.275 lb/in³
HP Alloys Nitronic® 60 Austenitic Stainless, Annealed
Annealed applies to tensile and/or hardness; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was originally designed as a high tempe..
Density 7.62 g/cc
0.275 lb/in³
HP Alloys Nitronic® 60 Austenitic Stainless, Level 4 Cold Worked
Level 4 Cold Worked applies to tensile properties of 0.25 to 2 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was origin..
Density 7.62 g/cc
0.275 lb/in³
HP Alloys Nitronic® 60 Austenitic Stainless, Level 5 Cold Worked
Level 5 Cold Worked applies to tensile properties of 0.25 to 1.5 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was orig..