Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe Lescalloy® 300M VAC-ARC High Strength Alloy Steel LESCALLOY 300M VAC-ARC steel is a modified 4340 steel with added silicon allowing for use of a higher tempering temperature. The steel has high hardenability and strength with good ductility and tou.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe Lescalloy® 4330+V VAC-ARC High Strength Alloy Steel LESCALLOY 4330+V VAC-ARC steel is a modification of 4330 steel with hardenability and other properties improved by the addition of vanadium. It is a low alloy steel capable of being heat treated to .. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe Lescalloy® 4335+V VAC-ARC High Strength Alloy Steel 4335+V VAC-ARC is a low alloy steel with good strength and high hardenability. In addition, uniform properties are obtained in large sections. The alloy can be heat treated to strength values with.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe Lescalloy® 4340 VAC-ARC ; 7.5" square High Strength Alloy Steel LESCALLOY 4340 VAC-ARC steel is a low alloy, nickel-chromium-molybdenum steel capable of being heat treated to high strength levels. The alloy has a good combination of ductility, toughness and str.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 17 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 9 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe LSSâ„¢ 4140 Alloy Steel (AISI 4140) TLS 4140 and 4142HT are versatile, alloy steels which are used in variety of tooling and other industrial applications. TLS 4140 is the classic AISI 4140 alloy steel which is sold in the annealed co.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe LSSâ„¢ 4142 Alloy Steel (AISI 4142) TLS 4140 and 4142HT are versatile, alloy steels which are used in variety of tooling and other industrial applications. TLS 4140 is the classic AISI 4140 alloy steel which is sold in the annealed co.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe CM-50â„¢ ASTM M50 High Speed Steel CM-50 is classified as an intermediate type high speed steel of the molybdenum chromium- vanadium variety. It is recommended for applications with moderate cutting conditions, such as woodworking to.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe Lescalloy® 4340 VAC-ARC ; 10.5" square High Strength Alloy Steel LESCALLOY 4340 VAC-ARC steel is a low alloy, nickel-chromium-molybdenum steel capable of being heat treated to high strength levels. The alloy has a good combination of ductility, toughness and str.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe Lescalloy® 6305 VAC-ARC ; High Strength Alloy Steel LESCALLOY 6305 VAC-ARC steel is a modified 4140 steel with higher molybdenum and a vanadium addition. The alloy steel is generally used in the 160/180,000 psi tensile strength range obtained with a.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
CeramTec Sonox® P53 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
CeramTec Sonox® P88 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Crucible Steel AISI 4340 Alloy Steel Information provided by Crucible Industries |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Crucible Steel KETOS® Tool Steel, AISI O1 Ketos is an oil-hardening tool steel which may be hardened from fairly low temperatures with little size change. This grade combines deep-hardening qualities with a fine-grained structure, affording.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Crucible Steel WR-95 Tool Steel, AISI H10 Modified WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight.. |
|||
Density | 7.83 g/cc @Temperature 399 °C |
0.283 lb/in³ @Temperature 750 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 23 (AISI M3:2) Hot Work Tool Steel Chromium-molybdenum-tungsten-vanadium alloyed PM steelVanadis 23 is a high speed powder metallurgical steel, recommended for low temperature die casting applications and warm forging applications wh.. |
|||
Density | 7.83 g/cc @Temperature 399 °C |
0.283 lb/in³ @Temperature 750 °F |
soft annealed |
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W .. |
|||
Density | 7.83 g/cc @Temperature 400 °C |
0.283 lb/in³ @Temperature 752 °F |
soft annealed condition |
Assab Steels ASP 60 Cold Work Steel ASP 60 is a W-Mo-V-Co alloyed PM high speed steel characterized by:Highest wear resistanceMaximum compressive strengthGood through hardening propertiesGood toughnessGood dimensional stability on hea.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
ATI Allvac® Vasco® 4340 Specialty Steel, Heat Treatment: 899°C (1650°F) Q+T Data provided by Allvac.Applications: Rocket motor cases, ordnance hardware, aircraft structural components, transmission gears, components, fasteners. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
ATI Allvac® Vasco® 450 Specialty Steel, Heat Treatment: 1038°C (1900°F) + Age Data provided by Allvac.Applications: Land-based turbine blades and buckets. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
ATI Allvac® Vasco® 9-4-30 Specialty Steel, Heat Treatment: 899°C (1650°F) + Age Data provided by Allvac.Applications: Aircraft structural components, rocket motor cases, pressure vessels, armor applications. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Carlson 303 Austenitic Stainless Steel Carlson 303 is an austenitic free-machining stainless steel. The standard 18-8 stainless steels are more difficult to turn, mill and drill which restricts their use when considerable machining is r.. |
|||
Density | 7.83 g/cc @Temperature 200 °C |
0.283 lb/in³ @Temperature 392 °F |
200 HB |
Assab Steels 760 Machinery Steel ASSAB 760 is an easily machinable carbon steel characterized by: Good machinabilityGood mechanical strengthASSAB 760 is primarily intended to be used in the as-delivered condition. It is only to be .. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Crucible Steel S7 XL (Premium AISI S7) Tool Steel Crucible S7XL is a double refined, high purity grade of S7. The remelt operation produces a cleaner steel with a more uniform microstructure, offering the following advantages over conventional S7:B.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Schmolz + Bickenbach Cryodur® 2312 (Brake Die) Cold Work Die Steel Description: Cryodur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared t.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Schmolz + Bickenbach Formadur® 2311 Plastic Mold Steel Description: Formadur® 2311 is a pre-hardened plastic mold steelCharacteristics: Good texturing compared to Formadur®2312 and Good polishability compared to Formadur® 231Applications: Injection m.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 6 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe LSS™ O1 Tool Steel (ASTM O1) TLS O1 tool steel is the original oil-hardening, "non-shrinking" tool steel that can be hardened to the Rockwell C 65 range from a low austenitizing temperature. TLS O1 is a general-purpose tool ste.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe LSS™ S7 Shock-Resisting Tool Steel (ASTM S7) TLS S7 Shock-Resisting tool steel is an air or oil hardening tool steel that is characterized by very high impact toughness. The combination of strength and high toughness makes S7 tool steel a cand.. |