Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe Lescalloy® 300M - HS VAC-ARC High Strength Alloy Steel LESCALLOY 300M-HS VAC-ARC steel is a modified 4340 steel with added silicon allowing for use of a higher tempering temperature. The steel has high hardenability and strength with good ductility and .. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe Lescalloy® 300M VAC-ARC High Strength Alloy Steel LESCALLOY 300M VAC-ARC steel is a modified 4340 steel with added silicon allowing for use of a higher tempering temperature. The steel has high hardenability and strength with good ductility and tou.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 17 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 9 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe LSSâ„¢ 4140 Alloy Steel (AISI 4140) TLS 4140 and 4142HT are versatile, alloy steels which are used in variety of tooling and other industrial applications. TLS 4140 is the classic AISI 4140 alloy steel which is sold in the annealed co.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe LSSâ„¢ 4142 Alloy Steel (AISI 4142) TLS 4140 and 4142HT are versatile, alloy steels which are used in variety of tooling and other industrial applications. TLS 4140 is the classic AISI 4140 alloy steel which is sold in the annealed co.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe Lescalloy® 4340 VAC-ARC ; 10.5" square High Strength Alloy Steel LESCALLOY 4340 VAC-ARC steel is a low alloy, nickel-chromium-molybdenum steel capable of being heat treated to high strength levels. The alloy has a good combination of ductility, toughness and str.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
CeramTec Sonox® P53 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Crucible Steel AISI 4340 Alloy Steel Information provided by Crucible Industries |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Crucible Steel KETOS® Tool Steel, AISI O1 Ketos is an oil-hardening tool steel which may be hardened from fairly low temperatures with little size change. This grade combines deep-hardening qualities with a fine-grained structure, affording.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Crucible Steel WR-95 Tool Steel, AISI H10 Modified WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight.. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
Bohler-Uddeholm BÖHLER M261 Extra Plastic Lens Mold Steel VACUUM ARC REMELTED HARDENED AND TEMPERED PLASTIC LENS MOLD STEELBOHLER M261 follow current trends in tool and die-making:Excellent machinability coupled with higher hardnessGood dimensional stabili.. |
|||
Density | 7.83 g/cc @Temperature 399 °C |
0.283 lb/in³ @Temperature 750 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 23 (AISI M3:2) Hot Work Tool Steel Chromium-molybdenum-tungsten-vanadium alloyed PM steelVanadis 23 is a high speed powder metallurgical steel, recommended for low temperature die casting applications and warm forging applications wh.. |
|||
Density | 7.83 g/cc @Temperature 399 °C |
0.283 lb/in³ @Temperature 750 °F |
soft annealed |
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W .. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
Carlson 2205 (UNS S31803) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
Carlson 2205 (UNS S32205) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
ATI Allvac® Vasco® 4340 Specialty Steel, Heat Treatment: 899°C (1650°F) Q+T Data provided by Allvac.Applications: Rocket motor cases, ordnance hardware, aircraft structural components, transmission gears, components, fasteners. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
ATI Allvac® Vasco® 9-4-30 Specialty Steel, Heat Treatment: 899°C (1650°F) + Age Data provided by Allvac.Applications: Aircraft structural components, rocket motor cases, pressure vessels, armor applications. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150M (Heated 760°C/2hr/AC then 621°C/4hr/AC) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 1150 AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |
|||
Density | 7.83 g/cc @Temperature 200 °C |
0.283 lb/in³ @Temperature 392 °F |
200 HB |
Assab Steels 760 Machinery Steel ASSAB 760 is an easily machinable carbon steel characterized by: Good machinabilityGood mechanical strengthASSAB 760 is primarily intended to be used in the as-delivered condition. It is only to be .. |
|||
Density | 7.83 g/cc @Temperature 400 °C |
0.283 lb/in³ @Temperature 752 °F |
|
Assab Steels ASP 23 Cold Work Steel ASP 23 is a chromium-molybdenum-tungsten-vanadium alloyed high speed steel which is characterized by:High wear resistance (abrasive profile)High compressive strengthVery good through-hardening prope.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Crucible Steel S7 XL (Premium AISI S7) Tool Steel Crucible S7XL is a double refined, high purity grade of S7. The remelt operation produces a cleaner steel with a more uniform microstructure, offering the following advantages over conventional S7:B.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Schmolz + Bickenbach Cryodur® 2312 (Brake Die) Cold Work Die Steel Description: Cryodur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared t.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Schmolz + Bickenbach Formadur® 2311 Plastic Mold Steel Description: Formadur® 2311 is a pre-hardened plastic mold steelCharacteristics: Good texturing compared to Formadur®2312 and Good polishability compared to Formadur® 231Applications: Injection m.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe LSS™ O1 Tool Steel (ASTM O1) TLS O1 tool steel is the original oil-hardening, "non-shrinking" tool steel that can be hardened to the Rockwell C 65 range from a low austenitizing temperature. TLS O1 is a general-purpose tool ste.. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe LSS™ S7 Shock-Resisting Tool Steel (ASTM S7) TLS S7 Shock-Resisting tool steel is an air or oil hardening tool steel that is characterized by very high impact toughness. The combination of strength and high toughness makes S7 tool steel a cand.. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
CeramTec Sonox® P51 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |
|||
Density | 7.83 g/cc | 0.283 lb/in³ | |
Latrobe LSS™ A6 Tool Steel (ASTM A6) TLS A6 tool steel is a medium-alloy, air-hardening tool steel that is characterized by its ability to be through hardened while using the low austenitizing temperatures which are typically associate.. |