Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.80 - 8.00 g/cc | 0.282 - 0.289 lb/in³ | |
Pacific Sintered Materials BZ-111-UC Yellow Brass Powdered Metal Applications: 80-20 leaded brass, coined for close dimensional control, strength and density.Equivalent MPIF Specification: CZP-2000-12All information provided by Pacific Sintered Metals. |
|||
Density | 7.80 - 8.00 g/cc | 0.282 - 0.289 lb/in³ | |
PSM Industries Pacific Sintered Metals Yellow Brass BZ-111-UC Powdered Metal 80-20 leaded brass, Coined for close dimensional control, strength and density Equivalent MPIF Specification: CZP-2000-12Information Provided by Pacific Sintered Metals, a division of PSM Industrie.. |