Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.53 g/cc | 0.308 lb/in³ | Theoretical |
Kennametal Stellite Deloro® 208 PM after P/M Processing Adhesive wear test data: cast 0.06 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, s.. |
|||
Density | 8.53 g/cc | 0.308 lb/in³ | Theoretical |
Kennametal Stellite Deloro® 208 PM cast Adhesive wear test data: cast 0.06 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, s.. |
|||
Density | 8.53 g/cc | 0.308 lb/in³ | Annealed |
Eagle Brass 260 Cartridge Brass, 1/2 Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Density | 8.53 g/cc | 0.308 lb/in³ | Annealed |
Eagle Brass 260 Cartridge Brass, 1/4 Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Density | 8.53 g/cc | 0.308 lb/in³ | Annealed |
Eagle Brass 260 Cartridge Brass, 3/4 Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Density | 8.53 g/cc | 0.308 lb/in³ | Annealed |
Eagle Brass 260 Cartridge Brass, Annealed Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Density | 8.53 g/cc | 0.308 lb/in³ | Annealed |
Eagle Brass 260 Cartridge Brass, Extra Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Density | 8.53 g/cc | 0.308 lb/in³ | Annealed |
Eagle Brass 260 Cartridge Brass, Extra Spring Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Density | 8.53 g/cc | 0.308 lb/in³ | Annealed |
Eagle Brass 260 Cartridge Brass, Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Density | 8.53 g/cc | 0.308 lb/in³ | Annealed |
Eagle Brass 260 Cartridge Brass, Spring Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Density | 8.53 g/cc | 0.308 lb/in³ | |
Chicago Extruded Metals BioBrass® UNS C26000 Copper-Zinc Alloy Finished product available as bar, wire, rod or tube.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Ext.. |
|||
Density | 8.53 g/cc | 0.308 lb/in³ | |
Wall Colmonoy COLMONOY® 227 Custom Formulated Nickel-Based Alloy For Glass Patented alloy specially designed for glass container mold protection and restoration. Also used for rebuilding automotive parts (clutch components).Method of Application: FusewelderInformation pro.. |
|||
Density | 8.53 g/cc | 0.308 lb/in³ | |
Weartech International WT-12 Cobalt Hardfacing & Wear Resistant Alloy Applications: extrusion dies, scissor blades, saw blades, guide bars, wood cutting tools, pump sleeves, twist rolls, knivesInformation provided by Weartech International |