Material Notes:
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particularly good spring material. The solderability of the alloy is severely impaired by its high zinc content.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.53 g/cc
0.308 lb/in³
Annealed
Mechanical Properties Metric English Comments
Hardness, Rockwell 30T 76 - 78
76 - 78
Thickness > 0.020 Inch
Tensile Strength, Ultimate 627 - 689 MPa
91000 - 100000 psi
Tensile Strength, Yield 565 - 627 MPa
82000 - 91000 psi
0.2% offset
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
in 2 in.
Tensile Modulus 110 GPa
16000 ksi
Thermal Properties Metric English Comments
CTE, linear 20.0 µm/m-°C

@Temperature 20.0 - 300 °C
11.1 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 121 W/m-K
840 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 70 %
70 %
Zinc, Zn 30 %
30 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed