Physical Properties Metric English Comments
Nitrogen Transmission 20.0 - 104 cc-mm/m²-24hr-atm
50.8 - 263 cc-mil/100 in²-24hr-atm
Average value: 32.0 cc-mm/m²-24hr-atm Grade Count:14
Overview of materials for Modified ETFE, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap..