Physical Properties Metric English Comments
Nitrogen Transmission 12.0 - 13.0 cc-mm/m²-24hr-atm
30.5 - 33.0 cc-mil/100 in²-24hr-atm
Average value: 12.5 cc-mm/m²-24hr-atm Grade Count:4
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Nitrogen Transmission 12.0 - 13.0 cc-mm/m²-24hr-atm
30.5 - 33.0 cc-mil/100 in²-24hr-atm
Average value: 12.5 cc-mm/m²-24hr-atm Grade Count:3
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Nitrogen Transmission 12.0 - 16.0 cc-mm/m²-24hr-atm
30.5 - 40.6 cc-mil/100 in²-24hr-atm
Average value: 13.1 cc-mm/m²-24hr-atm Grade Count:12
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Nitrogen Transmission 12.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
30.5 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
120 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® LED2643 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, ..
Nitrogen Transmission 12.0 - 16.0 cc-mm/m²-24hr-atm
30.5 - 40.6 cc-mil/100 in²-24hr-atm
Average value: 13.5 cc-mm/m²-24hr-atm Grade Count:20
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..