Polymer Property : Nitrogen Transmission = 40.6 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Nitrogen Transmission 12.0 - 16.0 cc-mm/m²-24hr-atm
30.5 - 40.6 cc-mil/100 in²-24hr-atm
Average value: 13.1 cc-mm/m²-24hr-atm Grade Count:12
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Nitrogen Transmission 12.0 - 16.0 cc-mm/m²-24hr-atm
30.5 - 40.6 cc-mil/100 in²-24hr-atm
Average value: 13.5 cc-mm/m²-24hr-atm Grade Count:20
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..