Polymer Property : Coating Weight = 0.0450 lb/ream Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 0.0720 g/m²
0.0450 lb/ream
DuPont Teijin Films Mylar® HR951 Polyester Film, 140 Gauge
Mylar® HR951 is a one-side release coated polyester film with good handling properties and clarity. It has been developed for use in various industrial applications.Information provided by DuPont.
Coating Weight 0.0720 g/m²
0.0450 lb/ream
DuPont Teijin Films Mylar® RSX951 Polyester Film, 105 Gauge
Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production..
Coating Weight 0.0720 g/m²
0.0450 lb/ream
DuPont Teijin Films Mylar® RSX951 Polyester Film, 120 Gauge
Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production..
Coating Weight 0.0720 g/m²
0.0450 lb/ream
DuPont Teijin Films Mylar® RSX951 Polyester Film, 140 Gauge
Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production..
Coating Weight 0.0720 g/m²
0.0450 lb/ream
DuPont Teijin Films Mylar® RSX951 Polyester Film, 175 Gauge
Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production..
Coating Weight 0.0720 g/m²
0.0450 lb/ream
DuPont Teijin Films Mylar® RSX951 Polyester Film, 48 Gauge
Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production..
Coating Weight 0.0720 g/m²
0.0450 lb/ream
DuPont Teijin Films Mylar® RSX951 Polyester Film, 92 Gauge
Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production..
Coating Weight 0.0720 g/m²
0.0450 lb/ream
DuPont Teijin Films Mylar® HR951 Polyester Film, 92 Gauge
Mylar® HR951 is a one-side release coated polyester film with good handling properties and clarity. It has been developed for use in various industrial applications.Information provided by DuPont.