Polymer Property : Linear Mold Shrinkage, Transverse = 0.0043 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0042 - 0.0043 cm/cm

@Thickness 2.00 mm
0.0042 - 0.0043 in/in

@Thickness 0.0787 in
ASTM D955
Solvay Specialty Polymers Amodel® FC-1150 Polyphthalamide (PPA), 50% Glass Fiber
Amodel® FC-1150 is an FDA-approved, 50% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h..
Linear Mold Shrinkage, Transverse 0.0029 - 0.0043 cm/cm

@Time 86400 sec
0.0029 - 0.0043 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE0021E PC
LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding, Flame Retardant, Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0029 - 0.0043 cm/cm

@Time 86400 sec
0.0029 - 0.0043 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE0021E PC (Asia Pacific)
LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0029 - 0.0043 cm/cm

@Time 86400 sec
0.0029 - 0.0043 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE0029EF PC
LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0029 - 0.0043 cm/cm

@Time 86400 sec
0.0029 - 0.0043 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE002ER PC
LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0029 - 0.0043 cm/cm

@Time 86400 sec
0.0029 - 0.0043 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE002ER PC (Asia Pacific)
LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0029 - 0.0043 cm/cm

@Time 86400 sec
0.0029 - 0.0043 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon DE002P PC
LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
Linear Mold Shrinkage, Transverse 0.0029 - 0.0043 cm/cm

@Time 86400 sec
0.0029 - 0.0043 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon DE002P PC (Asia Pacific)
LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..