Viscosity Measure 2.5 cSt
2.5 cSt
Kinetic/Kinematic
Dow Corning XIAMETER® PMCPPMX-0344 Cyclosiloxane Blend
Is chemically equivalent to DOW CORNING® 344 FLUID. A volatile methylsiloxane fluid, clear, odorless, VOC-exempt, low toxicity, low surface tension, evaporates completely at room temperatureInforma..
Viscosity Measure 2.5 cSt

@Temperature 25.0 °C
2.5 cSt

@Temperature 77.0 °F
Dow VORANATE™ T-80 toluene diisocyanate (TDI)
VORANATE™ T-80 TDI products are designed for a variety of high-resilience molding, TDI molding, formulating (systems) and flexible slabstock applications. They are used in the production of flexib..