Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.190 - 0.260 g/cc | 0.00686 - 0.00939 lb/in³ | |
Zircar Ceramics ASQ Castertip 14 pcf density refractory ceramic fiber "soft tip". Alumina bonding of shot free fiber results in extreme performance in manufacture of the finest grades of medical, food and packaging foils. Inform.. |