Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.00 - 2.10 g/cc | 0.0723 - 0.0759 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 130 Dense Refractory Castable Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values ap.. |
|||
Bulk Density | 2.00 - 2.10 g/cc | 0.0723 - 0.0759 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 140 GM Dense Refractory Castable Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this gunning castable can be applied up to 1400°C in slightly reducing atmospheres.Remarks: These values.. |
|||
Bulk Density | 2.00 - 2.10 g/cc | 0.0723 - 0.0759 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 145 F Sp Dense Refractory Castable Description: Curon 145F Special is a very fine graded castable and can be applied for the casting of complicated shapes.Remarks: These values apply to cast products. Also available in gunning variet.. |
|||
Bulk Density | 2.00 - 2.10 g/cc | 0.0723 - 0.0759 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 160 FS Dense Refractory Castable Description: This castable is based on fused silica. It has an extremely good thermal shock resistance and minor expansion behavior up to process temperature of 900°C. Application: zinc melting f.. |