Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.90 - 3.00 g/cc | 0.105 - 0.108 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 85 P Moldable Refractory Material Description: This phosphate bonded material based on corundum and bauxite has already at low temperature a reasonable strength and has a very good resistance against slag attack or liquid aluminum. .. |
|||
Bulk Density | 2.90 - 3.00 g/cc | 0.105 - 0.108 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 90 PF REPAIR Moldable Refractory Material Description: Curas 90 PF Repair ramming mix is especially developed for repairing purposes of Curas 90 PF linings. The product is supplied in two components: a dry powder and a liquid. Detailed inst.. |
|||
Bulk Density | 2.90 - 3.00 g/cc | 0.105 - 0.108 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS PBK D Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This moldable contains a phosphate binding agent and has a low silica cont.. |
|||
Bulk Density | 2.90 - 3.00 g/cc | 0.105 - 0.108 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS PBK DGM Moldable Refractory Material Description: This material is supplied as a dry gunning powder. This moldable contains a phosphate binding agent and has a low silica content. For a large variety of applications this results in goo.. |
|||
Bulk Density | 2.90 - 3.00 g/cc | 0.105 - 0.108 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 150 GZ (R) Dense Vibrating Refractory Castable Description: Vibron 150 GZ (R) is a low cement castable based on sintered South-American bauxite. The addition of zircon oxide in this product makes it suitable for areas under heavy chemical attack.. |
|||
Bulk Density | 2.90 - 3.00 g/cc | 0.105 - 0.108 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS PBK Moldable Refractory Material Description: This moldable contains a phosphate binding agent and has a low silica content. For a large variety of applications this results in a good slag resistance and high strength properties at.. |
|||
Bulk Density | 2.90 g/cc | 0.105 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics PCF (HS) Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Bulk Density | >= 2.90 g/cc | >= 0.105 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFCAST LC80 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Bulk Density | >= 2.90 g/cc | >= 0.105 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFCAST LC90ABR Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Bulk Density | >= 2.90 g/cc | >= 0.105 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics ZAP 010 Smart Cast Application Special Properties: High Strength CastableIndustry: Non-FerrousApplication: Aluminum Melting/Holding FurnaceInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Bulk Density | 2.90 g/cc | 0.105 lb/in³ | Self-flowing |
Stellar Canada CERAMITE® BKR-S Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |
|||
Bulk Density | 2.90 g/cc | 0.105 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics PCF (AZS) Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories C18A Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories C18B Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories C18C Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories C18CX Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories C18D Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories C18DX Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories FAM-1 Flame-Gunning Repair Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories FAM-2 Flame-Gunning Repair Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.90 g/cc | 0.105 lb/in³ | |
Chosun Refractories MCC-1 Magnesia Calcia Carbon Brick For Refining Ladle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.90 g/cc | 0.105 lb/in³ | |
Chosun Refractories SAL80C Special Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.90 g/cc | 0.105 lb/in³ | |
Chosun Refractories SAL85N Special Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories C18AX Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.90 g/cc | 0.105 lb/in³ | Powder |
Ametek P409L/409CB P/M Stainless Steel, Sintered from 6.00 g/cc Green Density P409L/409CB is a ferritic, weldable grade of stainless steel with high compressibility, enhanced green strength and good sinterability. This stabilized grade provides excellent corrosion resistance .. |
|||
Bulk Density | 2.90 g/cc | 0.105 lb/in³ | Powder |
Ametek P409L/409CB P/M Stainless Steel, Sintered from 6.45 g/cc Green Density P409L/409CB is a ferritic, weldable grade of stainless steel high compressibility, enhanced green strength and good sinterability. This stabilized grade provides excellent corrosion resistance and h.. |
|||
Bulk Density | 2.90 g/cc | 0.105 lb/in³ | Powder |
Ametek P409L/409CB P/M Stainless Steel, Sintered from 6.60 g/cc Green Density P409L/409CB is a ferritic, weldable grade of stainless steel with high compressibility, enhanced green strength and good sinterability. This stabilized grade provides excellent corrosion resistance .. |