Physical Properties Metric English Comments
Bulk Density 0.600 - 0.700 g/cc
0.0217 - 0.0253 lb/in³
Raschig Group PiMC 1221 High gloss
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa..
Bulk Density 0.600 - 0.700 g/cc
0.0217 - 0.0253 lb/in³
Raschig Group PiMC 1241 Sanitary, uni color
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa..
Bulk Density 0.600 - 0.700 g/cc
0.0217 - 0.0253 lb/in³
Raschig Group PiMC 1249 Sanitary, mix color
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa..
Bulk Density 0.600 - 0.700 g/cc
0.0217 - 0.0253 lb/in³
Raschig Group PiMC 1253 Highly flame retardant
This FR PiMC grade has been developed for top coats over M1 SMC/BMC grades. Such combinations will meet Europe’s most stringent FR tests for interiors of rolling stock, such as BS 476 and Spanish E..
Bulk Density 0.600 - 0.700 g/cc
0.0217 - 0.0253 lb/in³
Raschig Group PiMC 1841 Metallic colors
Adding metallic effect pigments to powder coatings gave rise to several application problems such as “spitting”. Synres-Almoco’s Metallic PiMC 1841 ensures easy processing and homogeneous surface..
Bulk Density 0.600 - 0.700 g/cc
0.0217 - 0.0253 lb/in³
Raschig Group PiMC 1949 Granite colors
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa..
Bulk Density 0.600 - 0.700 g/cc
0.0217 - 0.0253 lb/in³
DIN 53 468
Perstorp Compounds Aminel FX Melamine
Organically reinforced melamine material with excellent flow properties and high flexibility suitable for applications involving high complexity and surface demands.Information provided by Perstorp ..
Bulk Density 0.500 - 0.700 g/cc
0.0181 - 0.0253 lb/in³
Solvay Chemicals Ixper® 25M Magnesium Peroxide
IXPER® 25M is a Magnesium Peroxide powder used in a wide range of applications in environmental, and oil drilling e.g. markets. EINECS Number: 215-627-7/CAS Number: 1335-26-8Information provided ..
Bulk Density 0.600 - 0.700 g/cc
0.0217 - 0.0253 lb/in³
Powder Density; ISO 60
Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic
Carbon fiber reinforced phenolic moldable composite with superior tribological properties. High tensile and flexural strength and modulus combined with low density.Information provided by Vyncolit,..