Physical Properties Metric English Comments
Bulk Density 0.810 g/cc
0.0293 lb/in³
Poured; ASTM D1895
Eastman BD445 PET  (discontinued **)
Voridian Polymer BD445 is primarily targeted for the soft drink and water markets, it is also suitable for use in other beverage containers as well as food and on-food-related applications. This pol..
Bulk Density 0.810 g/cc
0.0293 lb/in³
Poured (Mexico Produced); ASTM D1895
Eastman CB12 PET  (discontinued **)
Voridian CB12 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. CB12 delivers fast, efficient processing and good ov..
Bulk Density 0.810 - 0.890 g/cc
0.0293 - 0.0322 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 125 R Refractory Insulating Castable
Description: Golite 125 R has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products. Also availa..
Bulk Density 0.810 g/cc
0.0293 lb/in³
ASTM D1895
Plenco 6343 Phenolic, Granular, Transfer Molded
PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz..
Bulk Density 0.810 g/cc
0.0293 lb/in³
DuPont™ Nomex® N196 Paper, 5 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Bulk Density 0.810 g/cc
0.0293 lb/in³
ASTM D1895
Plenco 1581 Polyester, Briquette, Transfer Molded
PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f..