Material Notes:
Voridian Polymer BD445 is primarily targeted for the soft drink and water markets, it is also suitable for use in other beverage containers as well as food and on-food-related applications. This polymer was formulated to provide improved efficiencies in preform and bottle production, a wide processing window, and very low acetaldehyde levels. This product is produced in Zarate, Argentina and will be supplied to customers in the Mercosur region.Applications/UsesBottlesFood packagingPackagingCarbonated soft drink containers
Physical Properties Metric English Comments
Bulk Density 0.810 g/cc
0.0293 lb/in³
Poured; ASTM D1895
0.871 g/cc
0.0315 lb/in³
Vibrated; ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
Crystalline Density; ASTM D1505
Melt Density 1.10 g/cc

@Temperature 285 °C
0.0397 lb/in³

@Temperature 545 °F
ASTM D1238
Particle Size 2500 µm
2500 µm
Pellet Size
Viscosity Measurement 0.80 - 0.84
0.80 - 0.84
Intrinsic; EMN-A-AC-G-V-1
Thermal Properties Metric English Comments
Heat of Fusion 58.0 J/g
25.0 BTU/lb
ASTM E793
Specific Heat Capacity 1.20 J/g-°C
0.287 BTU/lb-°F
ASTM E1269
1.50 J/g-°C

@Temperature 80.0 °C
0.359 BTU/lb-°F

@Temperature 176 °F
ASTM E1269
1.70 J/g-°C

@Temperature 100 °C
0.406 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
2.10 J/g-°C

@Temperature 280 °C
0.502 BTU/lb-°F

@Temperature 536 °F
ASTM E1269
Melting Point 241 °C
466 °F
Crystalline Peak Melting Point; ASTM D3418
Descriptive Properties Value Comments
Acetaldehyde <1ppm
TEPO-A-AN-G-GC-67
Color, CIE a* -3.3 to -0.3
VGAS-A-AN-G-RS-001
Color, CIE b* -3.1 to 0.9
VGAS-A-AN-G-RS-001
Color, CIE L* 74 min
VGAS-A-AN-G-RS-001
Fines, wt%, max 0.05
VGAS-A-AN-G-GA-1
Pellet Shape Cubical