Physical Properties Metric English Comments
Bulk Density 1.05 g/cc
0.0379 lb/in³
Nabaltec NABALOX® NO 652 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Bulk Density <= 1.05 g/cc
<= 0.0379 lb/in³
Magyar Aluminum ALOLT 2AF Aluminum Hydroxide
Ground type
Bulk Density 1.05 - 1.15 g/cc
0.0379 - 0.0415 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 1.2.4. MIX GM Refractory Insulating Castable
Description: This light weight gunning castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Re..
Bulk Density 1.05 - 1.15 g/cc
0.0379 - 0.0415 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE LW Refractory Insulating Castable
Description: This light weight (LW) castable can be used as a hot face material, as well as for the backlining of a dense castable or brickwork.Remarks: These values apply to cast products. Also ava..
Bulk Density 1.05 - 1.15 g/cc
0.0379 - 0.0415 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 120 Refractory Insulating Castable
Description: Golite 120 is composed of light weight aggregates, alumina cement and special additions to be sure of a high strength and a low firing shrinkage.Remarks: These values apply to cast prod..
Bulk Density 1.05 g/cc
0.0379 lb/in³
Powder Density; ISO 60
Vyncolit X655 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent dimensional stability and a very low coefficient of thermal expansion. UL listed.USES: Automotive disc brake pistons and gask..