Polymer Property : Bulk Density = 1.15 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.00 - 1.15 g/cc
0.0361 - 0.0415 lb/in³
Magyar Aluminum ALO-P95 Alumina
Alumina for Polishing
Bulk Density 1.05 - 1.15 g/cc
0.0379 - 0.0415 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 1.2.4. MIX GM Refractory Insulating Castable
Description: This light weight gunning castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Re..
Bulk Density 1.05 - 1.15 g/cc
0.0379 - 0.0415 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE LW Refractory Insulating Castable
Description: This light weight (LW) castable can be used as a hot face material, as well as for the backlining of a dense castable or brickwork.Remarks: These values apply to cast products. Also ava..
Bulk Density 1.05 - 1.15 g/cc
0.0379 - 0.0415 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 120 Refractory Insulating Castable
Description: Golite 120 is composed of light weight aggregates, alumina cement and special additions to be sure of a high strength and a low firing shrinkage.Remarks: These values apply to cast prod..