Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.60 g/cc | 0.0939 lb/in³ | |
MarkeTech Repton 214 Aluminum Oxide Brand 214 features: High porosity and purity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even wh.. |
|||
Bulk Density | 2.60 g/cc | 0.0939 lb/in³ | |
MarkeTech Repton 314 Mullite Brand 314 features: Superior hot creep.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when the.. |
|||
Bulk Density | 2.60 g/cc | 0.0939 lb/in³ | |
McDanel Advanced Ceramics MV-HR1 Mullite Mullite (3Al2O3 • 2SiO2) is a refractory oxide material combining low thermal expansion, good mechanical strength, and resilience at elevated temperatures. Mullite is formulated to produce den.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURASBOND 85 Moldable Refractory Material Description: Curasbond 85 is a pouring repairmass, characterized by excellent resistance to aluminum and rapid hardening. The product is supplied in two components: a dry powder and a liquid. It can.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 170 Dense Refractory Castable Description: A general purpose castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks: These v.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast FLUCON 160 K Dense Self Flowing Refractory Castable Description: Flucon 160 K is a self-flowing low cement castable based on silicon carbide. This castable is characterized by high strength high abrasion resistance and excellent thermal shock resista.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 160 Dense Vibrating Refractory Castable Description: Vibron 160 is a low cement vibrating castable on andalusite base, characterized by a high strength and excellent thermal shock resistance.Remarks: Indicated values apply to vibrated pro.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 170 M Dense Vibrating Refractory Castable Description: Vibron 170 is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid slags.Remar.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 170 M GS (R) Dense Vibrating Refractory Castable Description: Vibron 170 M GS (R) is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sl.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS SiC 70 D Moldable Refractory Material Description: This material is supplied as a dry powder and has to be mixed with clean potable water to the necessary consistency. Curas SiC 70D has a phosphate bond and is specially developed for b.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 160 K 50 Dense Vibrating Refractory Castable Description: Vibron 160 K 50 is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity, high abrasion resistance and a good oxidation resistance up to 1.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 162 K Sp Dense Vibrating Refractory Silicon Carbide Castable Vibron 162 K Sp is a low cement castable based on silicon carbide. This castable is characterized by a very good thermal conductivity, a high abrasion resistance and high resistance against oxidatio.. |
|||
Bulk Density | 2.60 g/cc | 0.0939 lb/in³ | |
Sharadaa Ceramics HA 70 High Alumina Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 2.60 g/cc | 0.0939 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics PCF60-1 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Bulk Density | 2.60 g/cc | 0.0939 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics PCF70 (M) Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Bulk Density | 2.60 g/cc | 0.0939 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics PCF70 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Bulk Density | >= 2.60 g/cc | >= 0.0939 lb/in³ | |
Sharadaa Ceramics PHOSTCAST 80 XL Phosphate Bonded Castables Description: We hold expertise in manufacturing a range of Phosphate Bonded Castables, that find wide application in boilers, power plant, refineries, foundries, rolling mills, forging furnaces and .. |
|||
Bulk Density | >= 2.60 g/cc | >= 0.0939 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFCAST LC60 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Bulk Density | 2.60 g/cc | 0.0939 lb/in³ | |
Sharadaa Ceramics MULL-SD Mullite Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 2.60 g/cc | 0.0939 lb/in³ | Scott |
China Tungsten YG15 Tungsten Carbide Powder Information provided by China Tungsten |
|||
Bulk Density | 2.60 g/cc | 0.0939 lb/in³ | Scott |
China Tungsten YG15C Tungsten Carbide Powder Information provided by China Tungsten |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | |
Chosun Refractories BP-95A Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | |
Chosun Refractories CUN-804 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.60 g/cc | 0.0939 lb/in³ | |
Chosun Refractories SB50 Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.60 g/cc | 0.0939 lb/in³ | |
Chosun Refractories SSBA Tube Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | >= 2.60 g/cc | >= 0.0939 lb/in³ | |
China-Yixing Longly Refractories Push Slab Semi-Corundum-Mullite Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractorine.. |
|||
Bulk Density | 2.60 - 2.65 g/cc | 0.0939 - 0.0957 lb/in³ | |
China-Yixing Longly Refractories Seggar SiC SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | |
China-Yixing Longly Refractories Slab SiC SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat.. |
|||
Bulk Density | 2.60 g/cc | 0.0939 lb/in³ | |
Chosun Refractories TD-S1 Special Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |