Gouda Vuurvast VIBRON 162 K Sp Dense Vibrating Refractory Silicon Carbide Castable

Category Ceramic , Carbide
Manufacturer Gouda Vuurvast
Trade Name VIBRON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast VIBRON 162 K Sp Dense Vibrating Refractory Silicon Carbide Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vibron 162 K Sp is a low cement castable based on silicon carbide. This castable is characterized by a very good thermal conductivity, a high abrasion resistance and high resistance against oxidation.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.60 - 2.70 g/cc
0.0939 - 0.0975 lb/in³
After drying at 110°C
Particle Size <= 3000 µm
<= 3000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
100 - 120 MPa

@Temperature 1400 °C
14500 - 17400 psi

@Temperature 2550 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 5.00 - 6.00 W/m-K

@Temperature 1400 °C
34.7 - 41.6 BTU-in/hr-ft²-°F

@Temperature 2550 °F
6.50 - 7.50 W/m-K

@Temperature 600 °C
45.1 - 52.0 BTU-in/hr-ft²-°F

@Temperature 1110 °F
7.00 - 8.00 W/m-K

@Temperature 100 °C
48.6 - 55.5 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Shrinkage -0.100 - 0.100 %

@Temperature 1400 °C
-0.100 - 0.100 %

@Temperature 2550 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 16 %
16 %
Fe2O3 0.20 %
0.20 %
SiC 77 %
77 %
SiO2 5.0 %
5.0 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 2600 kg
Mixing Water 4-4.5 liters
per 100 kgs dry material