Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.080 - 0.20 µm | 0.080 - 0.20 µm | outside diameter |
NanoAmor 95%; OD: 80-200 nm Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Particle Size | 0.080 - 0.20 µm | 0.080 - 0.20 µm | outside diameter |
NanoAmor 99.8%; OD: 80-200 nm Graphitized Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Particle Size | >= 0.080 µm | >= 0.080 µm | D<sub>50</sub> |
Heraeus Cleviosâ„¢ P VP AI 4083 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P VP AI 4083 is an antistatic material based o.. |
|||
Particle Size | 0.080 µm | 0.080 µm | |
American Elements Niobium Nanoparticles General DescriptionNiobium (Nb) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Niobium Particles are typically 10-20 nanometers (nm) with.. |
|||
Particle Size | 0.080 - 0.10 µm | 0.080 - 0.10 µm | |
American Elements Silicon Nanoparticles General DescriptionSilicon (Si) Nanoparticles, nanodots or Nanopowder are spherical high surface area metal particles. Nanoscale Silicon Particles are typically 5-25 nanometers (nm) with specific su.. |
|||
Particle Size | 0.080 µm | 0.080 µm | |
American Elements Tantalum Nanoparticles General DescriptionTantalum (Ta) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tantalum Particles are typically 10-20 nanometers (nm) wi.. |
|||
Particle Size | 0.080 µm | 0.080 µm | |
American Elements Tin Nanoparticles General DescriptionTin (Sn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tin Particles are typically 10-20 nanometers (nm) with specifi.. |