Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 9.0 - 11 µm
9.0 - 11 µm
Average
Malvern Minerals Trikup® PM Silane Treated Aluminum Hydroxide
Trikup® is a custom, silane treated alumina trihydrate or aluminum hydroxide. ATH is the largest volume flame retardant in the world. Trikup® adds additional functionality through the use of ..
Particle Size 7.0 - 11 µm
7.0 - 11 µm
Mean (agglomerates)
Momentive Performance Materials AC6003 Boron Nitride (BN) Powder
GE Advanced Ceramics boron nitride (BN) powders of grades HCV, AC6003, and AC6097 are agglomerates composed of submicron hexagonal turbostratic crystals. The mean particle size for these fine powder..
Particle Size 8.0 - 11 µm
8.0 - 11 µm
Mean particle size is 8 to 11 µm. Crystal size is 8 µm. %-325 mesh is 99.9%.
Momentive Performance Materials HCPL Boron Nitride (BN) Powder
All Grade HCP powders are high purity, fine (99%, -325 mesh), hexagonal Boron Nitride (BN). All exhibit the unique properties of BN in a form readily used in many advanced materials and processes. ..
Particle Size 7.0 - 11 µm
7.0 - 11 µm
Average Particle Size/Laser Diffraction D50
H.C. Starck Grade A Aluminum Nitride AIN
High thermally conductive ceramicsComposite ceramicsSiAlONsHeat sinksElectrically insulating packages for electronicsCrucibles for metals and salt meltsThermally conductive filler for polymersCompon..
Particle Size 7.0 - 11 µm
7.0 - 11 µm
Average Particle Size/Laser Diffraction D50
H.C. Starck Grade AT Aluminum Nitride AIN
High thermally conductive ceramicsComposite ceramicsSiAlONsHeat sinksElectrically insulating packages for electronicsCrucibles for metals and salt meltsThermally conductive filler for polymersCompon..
Particle Size 7.0 - 11 µm
7.0 - 11 µm
Mean
Carborundum CarboTherm™ CTL30 Boron Nitride Powder
Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect..
Particle Size 7.0 - 11 µm
7.0 - 11 µm
Mean particle size is 7 to 11 µm. Crystal size is 0.1 µm. %-325 mesh is 95%.
Momentive Performance Materials HCV Boron Nitride (BN) Powder
Grade HCV is a 95%, -325 mesh hexagonal Boron Nitride (BN) powder exhibiting the unique properties of BN in a form readily used in the production of many advanced materials. Grade HCV is an initial ..
Particle Size 5.0 - 11 µm
5.0 - 11 µm
average
Momentive Performance Materials PolarTherm® PT180 Boron Nitride (BN) Powder
Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen..