Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 1.5 - 3.0 µm | 1.5 - 3.0 µm | Laser Diffraction D50 |
H.C. Starck Grade II Amorphous Boron Automotive (igniter in airbags and belt tighteners)Additive in pyrotechnic mixtures (flares, igniters, and delay compositions)Additive in solid rocket propellant fuels and explosivesPreparation of r.. |
|||
Particle Size | 1.0 - 3.0 µm | 1.0 - 3.0 µm | Laser Diffraction D50 |
H.C. Starck High Vacuum 120 Titanium Carbide, TiC Hard metals (tooling and machining)CementsBlack ceramics, e.g. (Al2O3-TiC) |
|||
Particle Size | 2.0 - 3.0 µm | 2.0 - 3.0 µm | Average |
H.C. Starck High Vacuum 250 Titanium Carbide, TiC Hard metals (tooling and machining)CementsBlack ceramics, e.g. (Al2O3-TiC) |
|||
Particle Size | 1.0 - 3.0 µm | 1.0 - 3.0 µm | Laser Diffraction D50 |
H.C. Starck Standard 120 Titanium Carbide, TiC Hard metals (tooling and machining)CementsBlack ceramics, e.g. (Al2O3-TiC) |
|||
Particle Size | 2.0 - 3.0 µm | 2.0 - 3.0 µm | Average |
H.C. Starck Standard 250 Titanium Carbide, TiC Hard metals (tooling and machining)CementsBlack ceramics, e.g. (Al2O3-TiC) |
|||
Particle Size | 1.1 - 3.0 µm | 1.1 - 3.0 µm | d50 |
Indium Corp. Fine ITO Indium Tin Oxide Indium Tin Oxide (ITO, or tin-doped indium oxide) is a mixture of indium(III) oxide and tin(IV) oxide, typically 90% indium oxide, 10% tin oxide by weight. In powder form it is yellow-green in colo.. |
|||
Particle Size | 1.5 - 3.0 µm | 1.5 - 3.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade B Zirconium Diboride, ZrB2 Hot-pressed composites of excellent electrical conductivity, e.g., evaporation boats for continuous aluminum metallizingCrucible material for non-ferrous metalsCeramic shapes to be used in productio.. |
|||
Particle Size | 2.0 - 3.0 µm | 2.0 - 3.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade C Molybdenum Disilicide MoSi2 Composite ceramicsHeating elementsConstituent of glow plugs for enginesRaw material for MoSi2 sputter target (PVD) |
|||
Particle Size | 1.0 - 3.0 µm | 1.0 - 3.0 µm | Grain Size |
CoorsTek ACI-Co6 Tungsten Carbide Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries |
|||
Particle Size | 1.0 - 3.0 µm | 1.0 - 3.0 µm | Grain Size |
CoorsTek ACI-Ni6 Tungsten Carbide Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries |
|||
Particle Size | 2.0 - 3.0 µm | 2.0 - 3.0 µm | |
DayGlo Radiant® MP-Series Fluorescent microsphere pigments for plastics, solvent, bleed, and plate-out resistant fluorescent pigmentsApplications:Specialty Coatings/InksSolvent Sensitive SystemsPlate-out Resistant Plastic Co.. |
|||
Particle Size | 2.0 - 3.0 µm | 2.0 - 3.0 µm | Median Grain (d50) |
CeramTec 975 Alumina, 99.5% 975 (99.5%) offers unique technology by virtue of its optimal dispersion of the MgO phase with the alumina grains. With virtually no transgranular porosity in its microstructure, 975 exhibits high d.. |
|||
Particle Size | 2.0 - 3.0 µm | 2.0 - 3.0 µm | Median Grain (d50) |
CeramTec 977 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2 977 is a zirconia toughened alumina ceramic designed for use in ballistic protection and ceramic armor. |