Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 300 µm | <= 300 µm | 90% smaller than |
Nyco NYCOR® R Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | <= 300 µm | <= 300 µm | 90% smaller than |
Nyco NYGLOS® M50 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 300 µm | 300 µm | SABIC Method |
SABIC Innovative Plastics GELOY INP388 ASA+AMSAN SABIC INP388 is a high heat ASA resin, and is based on alphamethyl styrene acrylontrile butylacrylate styrene (AMS-ASA) and polybutyl arylate rubber. |
|||
Particle Size | 300 - 2500 µm | 300 - 2500 µm | Average value: 900 µm Grade Count:9 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Particle Size | <= 300 µm | <= 300 µm | sieve < 5% |
ICO Polymers ICOTEXâ„¢ 520-5016 300 Micron LDPE Powder Description: ICOTEX 520-5016 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and a .. |
|||
Particle Size | <= 300 µm | <= 300 µm | sieve < 5% |
ICO Polymers ICOTEXâ„¢ 520-5019 300 Micron LDPE Powder Description: ICOTEX 520-5019 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and a .. |
|||
Particle Size | 300 µm | 300 µm | Average Size |
Inhance Fluoro-Seal INHANCE® UH-1045 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Particle Size | 300 µm | 300 µm | Minimum of 95% less than |
H.C. Starck Ampersint® AISI 316 L 300 µm For P/M, HIP/CIP, MIM AISI 316 L is a type of low carbon austenitic Cr-Ni-Mo stainless steel with good oxidation resistance in intermittent service to 870°C and in continuous service to 925°C, resistance to intercr.. |
|||
Particle Size | 300 µm | 300 µm | Average Size |
Inhance Fluoro-Seal INHANCE® HD-1035 HDPE Product Description: INHANCE HD-1000 Series Polyethylene Particles are surface-activated High Density Polyethylene (HDPE) in particle or powder form. Surface activation makes the particles easy to.. |
|||
Particle Size | 300 µm | 300 µm | Maximum of 5% greater than |
H.C. Starck Amperit® 235.049 Calcined Bentonite coated with Nickel-Chromium-Aluminum |
|||
Particle Size | 300 - 600 µm | 300 - 600 µm | |
SPHERE ONE EXTENDOSPHERESâ„¢ 300/600 Hollow Spheres EXTENDOSPHERESâ„¢300/600 are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, they can .. |
|||
Particle Size | <= 300 µm | <= 300 µm | 0.2 |
Solvay REPEL-O-TEX® SRP-6 Polyethylene Glycol Polyester Description: Soil Release Polymer offering protection against the adhesion of greasy soils between two wash cycles. 100% active material in powder form.Chemical Name: POLYETHYLENE GLYCOL POLYESTERCA.. |
|||
Particle Size | 300 - 850 µm | 300 - 850 µm | 0.6 |
Solvay REPEL-O-TEX® SRP-6 Polyethylene Glycol Polyester Description: Soil Release Polymer offering protection against the adhesion of greasy soils between two wash cycles. 100% active material in powder form.Chemical Name: POLYETHYLENE GLYCOL POLYESTERCA.. |
|||
Particle Size | <= 300 µm | <= 300 µm | 98% min; TI-2087-2 |
Solvay RHEOZAN Biopolymer Description: Biopolymer: very stable in acid media (such as sulfuric acid). Highly pseudoplastic.Identification: SUCCINOGLYCAN GUMCAS: 73667 – 50 – 2Available in: Asia Pacific, Europe, Lat.. |
|||
Particle Size | >= 300 µm | >= 300 µm | <2%, 50 Mesh; TI-2087 |
Solvay RHODOPOL® 23 Surfactant Description: Rhodopol® 23 is Standard grade Xanthan Gum. It exhibits high pseudoplastic behavior and rapid hydration rate. This grade is registered on the FALCON list of approved substances.Ident.. |
|||
Particle Size | >= 300 µm | >= 300 µm | <2%, 50 Mesh; TI-2087 |
Solvay RHODOPOL® 50 MD Surfactant Description: Rhodopol® 50 MD is Xanthan Gum that turns into viscous colloidal solution on dispersion in water. It is It exhibits high pseudoplastic behavior effective thickening and stabilizing a.. |
|||
Particle Size | >= 300 µm | >= 300 µm | d90, 10%, vibrated sieving |
TIMCAL TIMREX® 50X100 mesh FR Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 300 µm | 300 µm | |
Dow Corning GP SHP 50 Dow Corning® SHP 50 Silicone Hydrophobic Powder was developed to offer the performance of a liquid silicon-based hydrophobic material in dry delivery systems. Dow Corning SHP 50 Silicone Hydrophobi.. |
|||
Particle Size | 300 - 400 µm | 300 - 400 µm | 0.15 |
Arkema Group OREVAC® 18732 Grafted Maleic Anhydride Polypropylene OREVAC 18732 and 18732P are maleic anhydride grafted polypropylene used in the manufacturing of multiplayer structures. These products are available in pellets or in powder. OREVAC 18732 and 18732P .. |
|||
Particle Size | 300 - 400 µm | 300 - 400 µm | 0.15 |
Arkema Group OREVAC® 18732P Grafted Maleic Anhydride Polypropylene OREVAC 18732 and 18732P are maleic anhydride grafted polypropylene used in the manufacturing of multiplayer structures. These products are available in pellets or in powder. OREVAC 18732 and 18732P .. |
|||
Particle Size | 300 µm | 300 µm | Average |
Azoty Tarnow™ TARFLEN SG-1 PTFE Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 300 - 430 µm | 300 - 430 µm | |
Potters Industries A-Series P-0170 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |