H.C. Starck Amperit® 552.072 Tungsten Carbide - Chromium Carbide-Nickel 73-20-7 (WC-CrC-Ni)

Category Ceramic , Carbide
Manufacturer H.C. Starck
Trade Name Amperit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 552.072 Tungsten Carbide - Chromium Carbide-Nickel 73-20-7 (WC-CrC-Ni).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Particle Size 11 - 16 µm
11 - 16 µm
10%
22 - 28 µm
22 - 28 µm
50%
26 - 32 µm
26 - 32 µm
MV
38 - 48 µm
38 - 48 µm
90%
62 µm
62 µm
Minimum of 95% less than
88 µm
88 µm
100% less than
Component Elements Properties Metric English Comments
Carbon, C 5.4 - 6.0 %
5.4 - 6.0 %
Chromium, Cr 19.5 - 24 %
19.5 - 24 %
Iron, Fe <= 0.80 %
<= 0.80 %
Nickel, Ni 6.0 - 7.5 %
6.0 - 7.5 %
Oxygen, O <= 0.20 %
<= 0.20 %
Tungsten, W 61.5 - 69.1 %
61.5 - 69.1 %