Polymer Property : Specific Surface Area = 1.5 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 1.5 m²/g
1.5 m²/g
BET
Nyco M325 WOLLASTOCOAT® Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
Specific Surface Area 1.5 m²/g
1.5 m²/g
BET
Nyco NYAD® 325 Wollastonite
Powdered grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particl..
Specific Surface Area 1.5 m²/g
1.5 m²/g
BET
Nyco NYGLOS® STPO Wollastonite
This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make..
Specific Surface Area 1.5 m²/g
1.5 m²/g
BET
Nabaltec APYRAL® 30X Al(OH)3
APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio..
Specific Surface Area 1.5 - 3.0 m²/g
1.5 - 3.0 m²/g
BET
Magyar Aluminum ALO-DN-2S Alumina
Reactive Alumina
Specific Surface Area 1.5 - 3.0 m²/g
1.5 - 3.0 m²/g
BET
Magyar Aluminum ALO-EL-2S Alumina
Reactive Alumina
Specific Surface Area 1.5 m²/g
1.5 m²/g
Imerys Minsparâ„¢ 250 Feldspar
Information provided by Imerys
Specific Surface Area 1.5 m²/g
1.5 m²/g
Zircar Zirconia ZYBF-4 Zirconia Bulk Fiber Insulation
Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed ..
Specific Surface Area 1.5 m²/g
1.5 m²/g
ATO 40-45-0 (BET)
Arkema Group ORGASOL® 2002 EXD Nat 1 Polyamide 12, Food Contact Approved
Information provided by Arkema Group
Specific Surface Area 1.5 m²/g
1.5 m²/g
ATO 40-45-0 (BET)
Arkema Group ORGASOL® 3202 D Nat 1 Copolyamide 6/12
Information provided by Arkema Group
Specific Surface Area 1.5 m²/g
1.5 m²/g
Zircar Zirconia ZYBF-4 Zirconia Bulk Fiber Insulation
Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed ..