Material Notes:
Reactive Alumina
Physical Properties Metric English Comments
Density 2.40 g/cc

@Pressure 100 MPa
0.0867 lb/in³

@Pressure 14500 psi
Green Density
3.30 g/cc

@Treatment Temp. 1600 °C,
Time 7200 sec
0.119 lb/in³

@Treatment Temp. 2910 °F,
Time 2.00 hour
Fired Density
Particle Size 1.7 - 2.5 µm
1.7 - 2.5 µm
d50
4.0 - 7.0 µm
4.0 - 7.0 µm
d90
Specific Surface Area 1.5 - 3.0 m²/g
1.5 - 3.0 m²/g
BET
Component Elements Properties Metric English Comments
Al2O3 >= 99.5 %
>= 99.5 %
Determined by difference
CaO <= 0.040 %
<= 0.040 %
Fe2O3 <= 0.050 %
<= 0.050 %
Na2O <= 0.10 %
<= 0.10 %
SiO2 <= 0.050 %
<= 0.050 %